Sterilizing medicinal ultrasonic coupling agent and preparation method thereof
An ultrasonic couplant, disinfection and sterilization technology, applied in pharmaceutical formulations, preparations for in vivo experiments, etc., can solve the problems of medical ultrasonic couplants that cannot achieve disinfection and sterilization, no medium, and inability to use disinfection.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0034] Example 1: Prepare a medical ultrasonic coupling agent with a total weight of 1000kg and a function of disinfection and sterilization.
[0035] The first step, take by weight 2% propylene glycol, 20kg, take by weight 2% glycerol, 20kg, be mixed with mixed solution;
[0036] In the second step, take 0.05% 2,4,4'-trichloro-2'-hydroxyl diphenyl ether, 1kg by weight percentage, and weigh 0.1% R-polysaccharide, 1kg by weight percentage, completely dissolve in the In the mixed solution made in one step, leave it;
[0037] The 3rd step, take by weight 0.6% cross-linked polyacrylic acid resin, 6kg, be dissolved in the distilled water of 350kg, obtain cross-linked polyacrylic acid resin solution;
[0038] In the fourth step, the mixed solution containing 2,4,4'-trichloro-2'-hydroxydiphenyl ether and R-polysaccharide in the second step is added to the cross-linked polyacrylic acid resin solution obtained in the third step under stirring , forming a gel-like macromolecular subst...
Embodiment 2
[0041] Example 2: Prepare a medical ultrasonic coupling agent with a total weight of 1000 kg and a function of disinfection and sterilization.
[0042]The first step, take by weight 5% propylene glycol, 50kg, take by weight 5% glycerol, 50kg, be mixed with mixed solution;
[0043] In the second step, take 0.19% 2,4,4'-trichloro-2'-hydroxyl diphenyl ether, 1.9kg by weight percentage, and weigh 1.0% R-polysaccharide, 10kg by weight percentage, completely dissolve in In the mixed solution made in the first step, leave it;
[0044] The 3rd step, take by weight percentage 1.0% cross-linked polyacrylic acid resin, 10kg, be dissolved in the distilled water of 300kg, obtain cross-linked polyacrylic acid resin solution;
[0045] In the fourth step, the mixed solution containing 2,4,4'-trichloro-2'-hydroxydiphenyl ether and R-polysaccharide in the second step is added to the cross-linked polyacrylic acid resin solution obtained in the third step under stirring , forming a gel-like mac...
Embodiment 3
[0048] Example 3: Prepare a medical ultrasonic coupling agent with a total weight of 1000 kg and a function of disinfection and sterilization.
[0049] The first step, take 7% propylene glycol, 70kg by weight percentage, take 7% glycerol, 70kg by weight percentage, be mixed with mixed solution;
[0050] In the second step, take 0.35% 2,4,4'-trichloro-2'-hydroxyl diphenyl ether, 3.5kg by weight percentage, and weigh 2.0% R-polysaccharide, 20kg by weight percentage, completely dissolve in In the mixed solution made in the first step, leave it;
[0051] The 3rd step, take by weight 1.5% cross-linked polyacrylic acid resin, 15kg, be dissolved in the distilled water of 300kg, obtain cross-linked polyacrylic acid resin solution;
[0052] In the fourth step, the mixed solution containing 2,4,4'-trichloro-2'-hydroxydiphenyl ether and R-polysaccharide in the second step is added to the cross-linked polyacrylic acid resin solution obtained in the third step under stirring , forming a ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com