Preparation method for pentadiene petroleum resin
A technology for petroleum resin and pentadiene, applied in the field of synthesizing piperylene petroleum resin, can solve the problems of affecting the quality and application of the resin, high labor intensity, pollution of the three wastes, etc., and achieves easy continuous production, easy production control, The effect of improving economic efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] Add solvent and boron trifluoride complex catalyst in proportion in reactor, then slowly drop piperylene concentrate (composition is shown in Table 1), catalyst and piperylene consumption ratio (weight) are 0.6, Control the rate of addition so that the reaction temperature is within 20°C. After the dropwise addition, the temperature was raised slowly, the reaction temperature was controlled at 20° C., and the reaction time was 10 h. After the reaction, deactivate with water, filter and use air stripping method to obtain the product piperylene petroleum resin, the resin yield reaches 82%, the hue (Fe—Co) can be obtained≤5, and the softening point is 89°C.
Embodiment 2
[0022] The experimental process and raw materials are the same as in Example 1, the catalyst to piperylene dosage ratio (weight) is 0.8, the reaction temperature is changed to 40° C., and the reaction time is 5 hours. After the reaction, unpolymer and solvent are flashed off to obtain the product piperylene petroleum resin with a resin yield of 84%, a hue (Fe-Co)≤4, and a softening point of 95°C.
Embodiment 3
[0024] The experimental process and raw materials are the same as in Example 1, the catalyst to piperylene dosage ratio (weight) is 0.5, the reaction temperature is changed to 50° C., and the reaction time is 6 hours. After the reaction is finished, unpolymer and solvent are flashed off to obtain the product piperylene petroleum resin with a resin yield of 88%, a hue (Fe-Co)≤4, and a softening point of 100°C.
PUM
Property | Measurement | Unit |
---|---|---|
softening point | aaaaa | aaaaa |
softening point | aaaaa | aaaaa |
softening point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com