Odor-free total-effect interior wall latex paint and preparation method thereof
A technology for interior wall latex paint and deodorization, applied in latex paint and coatings, can solve problems such as single functions, and achieve the effect of improving deodorization
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0035] A kind of odor-cleaning full-effect interior wall latex paint, the raw materials are by weight percentage, deionized water 22%-25%, cellulose 0.45-0.55%, defoamer 0.45%-0.55%, dispersant 0.5%-0.7%, color Filler 38%-41%, emulsion 33%-36%, fungicide 0.15%-0.25%.
[0036] The preparation method of described pure taste full-effect interior wall latex paint, comprises the following steps:
[0037] Step 1. Weigh the required deionized water, cellulose, defoamer, dispersant, pigment and filler, emulsion, and bactericide by weight percentage;
[0038] Step 2. First weigh 17-20% deionized water, put it into the stirring equipment, start stirring, add cellulose under slow stirring, and stir at a slow speed for 5 minutes to completely dissolve the cellulose particles;
[0039] Step 3. Adjust the speed of the stirring equipment to medium speed, add defoamer and dispersant under medium speed stirring, and stir for 2 minutes at medium speed;
[0040] Step 4. Add the pig...
Embodiment 2
[0043] A kind of odor-cleaning full-effect interior wall latex paint, the raw materials are according to the preferred weight percentage, deionized water 23%-24%, cellulose 0.45-0.50%, defoamer 0.45%-0.50%, dispersant 0.6%-0.7%, Pigment and filler 39%-40%, emulsion 34%-35%, fungicide 0.18%-0.22%.
[0044] The preparation method of described pure taste full-effect interior wall latex paint, comprises the following steps:
[0045] Step 1. Weigh the required deionized water, cellulose, defoamer, dispersant, pigment and filler, emulsion, and bactericide by weight percentage;
[0046] Step 2. First weigh 17-20% deionized water, put it into the stirring equipment, start stirring, add cellulose under slow stirring, and stir at a slow speed for 5 minutes to completely dissolve the cellulose particles;
[0047] Step 3. Adjust the speed of the stirring equipment to medium speed, add defoamer and dispersant under medium speed stirring, and stir for 2 minutes at medium speed; ...
Embodiment 3
[0051] A kind of odor-cleaning full-effect interior wall latex paint, the raw materials are according to the optimal weight percentage, deionized water 23.20%, cellulose 0.50%, defoamer 0.50%, dispersant 0.60%, pigment and filler 40%, emulsion 35%, bactericidal Agent 0.20%.
[0052] The preparation method of described pure taste full-effect interior wall latex paint, comprises the following steps:
[0053] Step 1. Weigh the required deionized water, cellulose, defoamer, dispersant, pigment and filler, emulsion, and bactericide by weight percentage;
[0054] Step 2. First weigh 18.20% deionized water, put it into the stirring equipment, start stirring, add cellulose under slow stirring, and stir at slow speed for 5 minutes to completely dissolve the cellulose particles;
[0055] Step 3. Adjust the speed of the stirring equipment to medium speed, add defoamer and dispersant under medium speed stirring, and stir for 2 minutes at medium speed;
[0056] Step 4. Add th...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology