Embodiment 1
[0047] Mix epoxy resin, polyurethane, dibutyl phthalate, m-cresol and react at room temperature for 3 hours to obtain the first mixture; mix polyamine, salicylic acid and polyethylene glycol After reacting for 3 hours, the second mixture was obtained; after mixing the first mixture and the second mixture, adding quartz sand and PO42.5 cement, mixing and stirring evenly to obtain epoxy grouting glue for bonding sound barrier columns.
[0048] Among them, by weight, 5 parts of epoxy resin, 1 part of polyurethane, 0.5 part of dibutyl phthalate, 1 part of m-cresol, 2 parts of polyamine, 0.2 part of salicylic acid, 0.5 part of polyethylene glycol , 70 parts of quartz sand, 10 parts of PO42.5 cement.
Embodiment 2
[0050] Mix epoxy resin, polyurethane, dibutyl phthalate, and m-cresol and react at room temperature for 10 hours to obtain the first mixture; mix polyamine, salicylic acid, and polyethylene glycol After reacting for 10 hours, the second mixture was obtained; after mixing the first mixture and the second mixture, adding quartz sand and PO42.5 cement, mixing and stirring evenly to obtain epoxy grouting glue for bonding sound barrier columns.
[0051] Among them, by weight, 10 parts of epoxy resin, 5 parts of polyurethane, 1 part of dibutyl phthalate, 3 parts of m-cresol, 6 parts of polyamine, 0.8 part of salicylic acid, and 1 part of polyethylene glycol , 90 parts of quartz sand, 30 parts of PO42.5 cement.
Embodiment 3
[0053] Mix epoxy resin, polyurethane, dibutyl phthalate, m-cresol and react at room temperature for 5 hours to obtain the first mixture; mix polyamine, salicylic acid and polyethylene glycol After reacting for 5 hours, the second mixture was obtained; after mixing the first mixture and the second mixture, adding quartz sand and PO42.5 cement, mixing and stirring evenly to prepare epoxy grouting glue for bonding the sound barrier column.
[0054] Among them, by weight, 7 parts of epoxy resin, 2 parts of polyurethane, 0.6 part of dibutyl phthalate, 2 parts of m-cresol, 3 parts of polyamine, 0.4 part of salicylic acid, 0.6 part of polyethylene glycol , 75 parts of quartz sand, 15 parts of PO42.5 cement.
PUM
Property | Measurement | Unit |
---|---|---|
compressive strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com