Sn/Sb-GAC (granular activated carbon) particle and application thereof to treating 4-chlorophenol waste water through three-dimensional electrochemical reaction
A technology of chemical reaction and three-dimensional electricity, applied in the direction of sterilization/microdynamic water/sewage treatment, water/sewage treatment, water/sewage treatment equipment, etc., can solve the problems of high removal cost, limited removal rate, and difficult removal , to achieve good adsorption effect, simple operation, and increase the area
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation Embodiment 1
[0029] (1) Pretreatment of granular activated carbon: boil the granular activated carbon with a large amount of deionized water, dry it, and set aside.
[0030] (2) Weigh SnCl in turn according to the mass ratio: 8:0.4:60 4 ·5H 2 O, SbCl 3 and the GAC.
[0031] (3) SnCl 4 ·5H 2 O, SbCl3 Dissolve in an organic alcohol solvent to obtain a mixed solution, then soak GAC in the mixed solution, and shake on a shaking table at 150r / min for 2 hours to obtain the crude product of supported Sn / Sb-GAC particles, then dry and roast at 300°C to obtain the loaded type Sn / Sb–GAC particles.
preparation Embodiment 2
[0033] (1) Pretreatment of granular activated carbon: boil the granular activated carbon with a large amount of deionized water, dry it, and set aside.
[0034] (2) According to the mass ratio: 10:1:65, weigh SnCl in sequence 4 ·5H 2 O, SbCl 3 and the GAC.
[0035] (3) SnCl 4 ·5H 2 O, SbCl 3 Dissolve in an organic alcohol solvent to obtain a mixed solution, then soak GAC in the mixed solution, and shake on a shaking table at 160r / min for 3 hours to obtain the crude product of supported Sn / Sb-GAC particles, then dry and roast at 350°C to obtain the loaded type Sn / Sb–GAC particles.
preparation Embodiment 3
[0037] (1) Pretreatment of granular activated carbon: boil the granular activated carbon with a large amount of deionized water, dry it, and set aside.
[0038] (2) Weigh SnCl in turn according to the mass ratio: 12:1.5:70 4 ·5H 2 O, SbCl 3 and the GAC.
[0039] (3) SnCl 4 ·5H 2 O, SbCl 3 Dissolve in an organic alcohol solvent to obtain a mixed solution, then soak GAC in the mixed solution, and shake on a shaking table at 170r / min for 4 hours to obtain the crude product of supported Sn / Sb-GAC particles, then dry and roast at 400°C to obtain the loaded type Sn / Sb–GAC particles.
PUM
Property | Measurement | Unit |
---|---|---|
electric potential / voltage | aaaaa | aaaaa |
clearance rate | aaaaa | aaaaa |
decolorization rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com