Embodiment 1
[0023] figure 1 It is a schematic flowchart of a control method for heating power output mode of a continuous annealing furnace in an embodiment of the present invention. Such as figure 1 As shown, the method includes:
[0024] Step 1: Obtain the total column number N of radiant tubes in the heating section of the continuous annealing furnace, and obtain the output power P of the i-th column radiant tubes i , where P i The range is 0≤P i ≤100, the value range of i is 1~N;
[0025] Specifically, the total number of rows of radiant tubes in the heating section of the continuous annealing furnace is N, and the output power of the i-th row of radiant tubes is P i , then the power range of each row of radiant tubes satisfies 0≤P i ≤100, where i ranges from 1 to N. The specification of the strip steel is used as the control quantity of the power output mode, that is, according to the strip steel width w and the strip steel thickness h as the control quantity of the power outp...
Embodiment 2
[0036] A control method of a continuous annealing furnace heating power output mode of the present invention is described in detail below, specifically as follows:
[0037] Taking the 2230 continuous annealing production line of a certain factory as an example, considering the actual parameters of the heating section of the continuous annealing furnace, the total number of radiant tubes is N=31, and according to the actual production data of the production line, the coefficient of influence degree of aspect ratio is determined to be a=2.6, and the aspect ratio benchmark Value b=950, when the PID output power is 90%, then according to the width-thickness ratio of the strip w / h When the width-to-thickness ratio of the strip steel w / h≥950, then
[0038] When w / h=1450, for example w=1450mm, h=1.0mm, such as figure 2 As shown, the heating curve form is similar to the Normal mode;
[0039] When w / h=950, for example w=950mm, h=1.0mm, such as image 3 As shown, the heating curve ...