Embodiment 1
[0027] Each 10kg icodextrin dressing contains: icodextrin 0.3kg, purified water 9.2kg, 1,3-butanediol 0.4kg, hydrolyzed sclerotin gum 0.05kg, phenoxyethanol 0.02kg, and methyl paraben 0.03 kg.
[0028] The preparation process of the dressing is as follows: icodextrin, hydrolyzed sclerotin gum, methyl paraben, and 1,3-butanediol are dissolved in purified water and heated to 85°C, stirred evenly, kept warm for 30 minutes and then cooled to below 45°C , Add phenoxyethanol. The liquid dressing of Ecodextrin is obtained after standing and defoaming.
Embodiment 2
[0030] Each 10kg icodextrin dressing contains: icodextrin 0.37kg, purified water 9.0kg, 1,2-pentanediol 0.2kg, 1,3-propanediol 0.3kg, polyethylene glycol-115M 0.06kg, phenoxy 0.05 kg of ethanol and 0.02 kg of methyl paraben.
[0031] The preparation process of the dressing is as follows: Dissolve 1,2-pentanediol and 1,3-propanediol in purified water, add icodextrin, polyethylene glycol-115M, stir well, heat to 36.5℃ and add phenoxyethanol , Methyl paraben, stir evenly, leave it to stand for defoaming, and obtain an icodextrin dressing (essence).
Embodiment 3
[0033] Each 10kg icodextrin dressing contains: icodextrin 0.25kg, purified water 9.4kg, 1,2-propanediol 0.1kg, dipropylene glycol 0.1kg, acryloyldimethyl taurine ammonium / VP copolymer 0.05 kg, DMDM hydantoin 0.1kg.
[0034] The preparation process of the dressing is as follows: Dissolve 1,2-propylene glycol and dipropylene glycol in purified water, add icodextrin, ammonium acryloyldimethyl taurate / VP copolymer, stir well, and heat to 35°C Add DMDM hydantoin, stir evenly, and leave it to stand for defoaming to obtain an icodextrin liquid dressing.
[0035] Implementation Effect:
[0036] (1) After high temperature sterilization of the dressings obtained in the above examples, they were all sealed and allowed to stand for one week at normal temperature and pressure, and the state of the auxiliary materials was observed every 6 hours. The obtained dressings were in stable state without flocculation or agglomeration.
[0037] (2) Take 18 rats, apply or spray the dressing obtained in ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com