Examples
Embodiment 1
[0031] Embodiment one: a kind of manufacture method of reflective oil paint for fine arts of the present invention adopts the following process steps, and its formula ratio is counted in parts by mass:
[0032] First add 0.5 parts of beeswax and 15 parts of sunflower seed salad oil to 30 parts of refined linseed oil, heat to 85°C, stir until completely dissolved; cool to 40°C, add 2-ethyl alcohol cobalt (CAS#13586- 82-8) 0.3 parts, 0.6 parts of butyl-p-cresol, and 0.3 parts of phenoxyethanol were stirred evenly to make an adhesive. Add 2930 parts of pigment powder CI Pigment Blue to the binder and stir well, then add 18 parts of lithopone, 8 parts of silicon dioxide hydrate, 0.8 parts of aluminum stearate, 12 parts of aluminum hydroxide and stir evenly to form a coarse slurry. The coarse slurry was added to the hopper of a three-roll mill and ground for 5 times through the three-roll mill; the diameter of the three-roll mill rolls was 650 mm, and the speed of the three rolls ...
Embodiment 2
[0033] Embodiment two: a kind of manufacture method of reflective oil paint for fine arts of the present invention adopts the following process steps, and its formula ratio is counted by mass parts:
[0034] First add 0.4 parts of beeswax and 12 parts of sunflower seed salad oil to 28 parts of refined linseed oil, heat to 88°C, stir until completely dissolved; cool to 43°C, add 2-ethyl alcohol cobalt (CAS#13586- 82-8) 0.4 parts, 0.5 parts of butyl-p-cresol, and 0.4 parts of phenoxyethanol were stirred evenly to make an adhesive. Add 20 parts of pigment powder copper phthalocyanine blue to the binder and stir well, then add 20 parts of lithopone, 7 parts of silicon dioxide hydrate, 0.6 parts of aluminum stearate and 14 parts of aluminum hydroxide and stir evenly to form a Coarse stock. The coarse slurry was added to the hopper of a three-roll mill and ground for 5 times through the three-roll mill; the diameter of the three-roll mill rolls was 650 mm, and the speed of the thre...
Embodiment 3
[0035] Embodiment three: a kind of manufacture method of reflective oil paint for art of the present invention adopts the following process steps, and its formula ratio is counted by mass parts:
[0036] First add 0.5 parts of beeswax and 15 parts of sunflower seed salad oil to 32 parts of refined linseed oil, heat the temperature to 90°C, stir until completely dissolved; cool to 45°C, add 2-ethyl alcohol cobalt (CAS#13586- 82-8) 0.2 parts, 0.4 parts of butyl-p-cresol, and 0.35 parts of phenoxyethanol were stirred evenly to make an adhesive. Add 17035 parts of pigment powder CI Pigment Red to the binder and stir well, then add 22 parts of lithopone, 6 parts of silicon dioxide hydrate, 0.8 parts of aluminum stearate, 10 parts of aluminum hydroxide and stir evenly to form a coarse slurry. The coarse slurry was added to the hopper of a three-roll mill and ground for 5 times through the three-roll mill; the diameter of the three-roll mill rolls was 650 mm, and the speed of the th...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com