Embodiment 1
[0036] Dissolve 4g of carboxymethyl chitosan in 100ml of distilled water and stir for 1 hour, then add 4g of gelatin and stir for 2 hours, then add 1g of glycerin and stir for 2 hours, then add hyaluronic acid and stir for 2 hours, and finally slowly add 1.25g of 5- Aminolevulinic acid hydrochloride was stirred until dissolved. After standing until there are no air bubbles, pour it into the stereotyped mold at -40°C for 4 hours, freeze-dry it for 4 hours, raise the temperature to minus 10°C and maintain it for 16 hours, then raise the temperature to 20°C for 3 hours, and shape it. Nearly 50 structures such as figure 2 The single-layer drug delivery stent.
Embodiment 2
[0038] Dissolve 4g of carboxymethyl chitosan in 100ml of distilled water and stir for 1 hour, then add 4g of gelatin and stir for 2 hours, then add 1g of glycerin and stir for 2 hours, then add hyaluronic acid and stir for 2 hours, and finally slowly add 2.5g of 5 - Aminolevulinic acid hydrochloride was stirred until dissolved. After standing until there are no air bubbles, pour it into the stereotyped mold at -40°C for 4 hours, freeze-dry it for 4 hours, raise the temperature to minus 10°C and maintain it for 16 hours, then raise the temperature to 20°C for 3 hours, and shape it. Nearly 50 structures such as figure 2 The single-layer drug delivery stent.
Embodiment 3
[0040] Dissolve 0.2g of carboxymethyl chitosan in dichloromethane, pour it into the shaping mold, freeze-dry for 6 hours and put it into a special shaping mold as the inner layer; then dissolve 4g of carboxymethyl chitosan in 100ml of distilled water After stirring for 1 hour, add 4g of gelatin and stir for 2 hours, then add 1g of glycerin and stir for 2 hours, then add hyaluronic acid and stir for 2 hours, and finally add 15g of 5-aminolevulinic acid hydrochloride slowly and stir until dissolved. After standing still until there are no air bubbles, pour it into the shaping mold, freeze at -40°C for 4 hours, raise the temperature to minus 10°C for 16 hours, and raise the temperature to 20°C for 3 hours, and form a composite layer with the inner layer, making nearly 50 structures such as image 3 The composite layer drug delivery stent.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com