Decorative fabric and production process thereof
A production process and fabric technology, applied in fabrics, dyeing methods, textiles, etc., can solve the problems of no comfort, no environmental protection characteristics, etc., and achieve the effects of unique effect surface, good moisture absorption, and large friction coefficient
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The utility model relates to a decorative fabric, the warp thread is made of polyester glossy yarn, and the weft thread is made of gold and silver thread, chenille yarn and tape yarn with a weight ratio of 2:5:3. Among them, the specification of polyester bright yarn is 150 D , the gauge of gold and silver wire is 170 D , the chenille yarn is 5.5 stick / eye chenille yarn, and the specification of tape yarn is 1200 D , and the warp density of the decorative fabric is 64 threads / cm, and the weft density is 26 threads / cm.
[0026] The production process of the decorative fabric includes the following steps: warp and weft dyeing → warping → machine weaving → gray cloth inspection → gray cloth rolling → cloth seaming → washing, dyeing and finishing → softening treatment → finished product shaping. Among them, the water temperature in the washing, dyeing and finishing process is controlled at 70°C; the softener used in the softening process is amino silicone microemulsion; t...
Embodiment 2
[0030] The utility model relates to a decorative fabric, the warp thread is made of polyester glossy yarn, and the weft thread is made of gold and silver thread, chenille yarn and tape yarn with a weight ratio of 2:5:3. Among them, the specification of polyester bright yarn is 150 D , the gauge of gold and silver wire is 170 D , the chenille yarn is 5.5 stick / eye chenille yarn, and the specification of tape yarn is 1200 D , and the warp density of the decorative fabric is 64 threads / cm, and the weft density is 26 threads / cm.
[0031] The production process of the decorative fabric includes the following steps: warp and weft dyeing → warping → machine weaving → gray cloth inspection → gray cloth rolling → cloth seaming → washing, dyeing and finishing → softening treatment → finished product shaping. Among them, the water temperature in the washing, dyeing and finishing process is controlled at 72°C; the softener used in the softening process is amino silicone microemulsion; t...
Embodiment 3
[0035]The utility model relates to a decorative fabric, the warp thread is made of polyester glossy yarn, and the weft thread is made of gold and silver thread, chenille yarn and tape yarn with a weight ratio of 2:5:3. Among them, the specification of polyester bright yarn is 100 D , the gauge of gold and silver wire is 160 D , the chenille yarn is viscose / polyester chenille yarn of 4.5 counts, and the specification of the tape yarn is 1500 D , and the warp density of the decorative fabric is 64 threads / cm, and the weft density is 26 threads / cm.
[0036] The production process of the decorative fabric includes the following steps: warp and weft dyeing → warping → machine weaving → gray cloth inspection → gray cloth rolling → cloth seaming → washing, dyeing and finishing → softening treatment → finished product shaping. Among them, the water temperature in the washing, dyeing and finishing process is controlled at 75°C; the softener used in the softening process is amino sili...
PUM
Property | Measurement | Unit |
---|---|---|
Specification | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com