[0017] S1: Wash the trimmed Tan sheepskin in water for 20 minutes, and then place it in a degreasing solution for degreasing treatment; control the degreasing treatment time to 50 minutes, the temperature is 40-45 ° C, and the degreasing agent used in the degreasing treatment is 17 Octyl polyoxyethylene ether in parts by weight, polyvinyl alcohol in 5 parts by weight, octadecyl dimethyl ammonium oxide in 8 parts by weight, triethanolamine in 5 parts by weight and water of 65 parts by weight are mixed to form, degreasing agent and Water is mixed according to 1:3.
[0018] S2: Wash the degreased sheepskin with water and place it in a tanning solution for 50 minutes at 42-45°C. The tanning agent used consists of 5 parts by weight of boron powder and chromium trioxide according to (boron powder and chromium trioxide According to mixing according to the weight ratio of 1:9), the mixture of mixing composition, the resin retanning agent of 4 parts by weight, the acid-resistant fatliq...
Embodiment 2
[0023] S1: Wash the trimmed Tan sheepskin in water for 10 minutes, and then place it in a degreasing solution for degreasing treatment; control the degreasing treatment time to 40 minutes, and the temperature is 40-45°C. The degreasing agent used in the degreasing process consists of 17 parts by weight of octyl polyoxyethylene ether, 5 parts by weight of polyvinyl alcohol, 8 parts by weight of octadecyl dimethyl ammonium oxide, 5 parts by weight of triethanolamine and 65 parts by weight of The composition of the water mixture, the degreaser and water are mixed according to 1:3,
[0024] S2: Wash the degreased sheepskin with water and place it in a tanning solution for 50 minutes at 42-45°C. The tanning agent used consists of 7 parts by weight of boron powder and chromium trioxide (boron powder and chromium trioxide according to 1:9 weight ratio for mixing) mixture of mixing composition, 4 parts by weight of resin retanning agent, 2 parts by weight of acid-resistant fatliquorin...
Embodiment 3
[0029] S1: The trimmed Tan sheepskin is soaked in water for 15 minutes, and then placed in a degreasing solution for degreasing treatment; the degreasing treatment time is controlled to be 50 minutes, and the temperature is 45°C. The degreasing agent used in the degreasing process consists of 17 parts by weight of octyl polyoxyethylene ether, 5 parts by weight of polyvinyl alcohol, 8 parts by weight of octadecyl dimethyl ammonium oxide, 5 parts by weight of triethanolamine and 65 parts by weight of The composition of the water mixture, the degreaser and water are mixed according to 1:3,
[0030] S2: Wash the degreased sheepskin with water and place it in a tanning solution at 42°C for 55 minutes. The tanning agent used is 6 parts by weight of boron powder and chromium trioxide (boron powder and chromium trioxide according to the ratio of 1: 8 weight ratio) mixture of composition, 3 parts by weight of resin retanning agent, 3 parts by weight of acid-resistant fatliquoring agent...