A kind of nanoemulsion insecticide and preparation method thereof
A technology of insecticide and nanoemulsion, which is applied in the field of pesticides, can solve the problems of weak insecticidal effect, damage to the ecosystem, and poor persistence of drug effect, and achieve strong insecticidal effect, simple process, and low destructive effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] Party:
[0020] Cyhalothrin 1g, spinosad 0.1g, matrine 0.2g, nano titanium dioxide 10g, soybean oil 200g, egg yolk lecithin 50g, n-butanol 10g, Tween 800.1g.
[0021] Preparation:
[0022] (1) Cyhalothrin, spinosad, egg yolk lecithin and Tween 80 are added to soybean oil, mixed evenly, to obtain an oil phase solution;
[0023] (2) under stirring conditions, the above-mentioned oil phase solution is added into water to obtain an oil-water mixture;
[0024] (3) Add n-butanol, matrine and nano-titanium dioxide into water to dissolve, slowly add it dropwise into the above-mentioned oil-water mixture, and control the temperature of the oil-water mixture to be 30°C;
[0025] (4) After the dropwise addition, 200W ultrasonic for 5min, the solution is transparent, that is to say.
[0026] The average particle diameter of the obtained nanoemulsion insecticide is 60nm.
Embodiment 2
[0028] Party:
[0029] Cyhalothrin 1g, spinosad 0.5g, matrine 0.8g, nano titanium dioxide 20g, soybean oil 300g, egg yolk lecithin 70g, n-butanol 16g, Tween 800.5g.
[0030] Preparation:
[0031] (1) Cyhalothrin, spinosad, egg yolk lecithin and Tween 80 are added to soybean oil, mixed evenly, to obtain an oil phase solution;
[0032] (2) under stirring conditions, the above-mentioned oil phase solution is added into water to obtain an oil-water mixture;
[0033] (3) Add n-butanol, matrine and nano-titanium dioxide into water to dissolve, slowly add it dropwise into the above-mentioned oil-water mixture, and control the temperature of the oil-water mixture to be 40°C;
[0034] (4) After the dropwise addition, 400W ultrasonic for 15min, the solution is transparent, and it is ready.
[0035] The average particle diameter of the obtained nanoemulsion insecticide is 80nm.
Embodiment 3
[0037] Party:
[0038] Cyhalothrin 1g, spinosad 0.3g, matrine 0.5g, nano-titanium dioxide 15g, soybean oil 250g, egg yolk lecithin 60g, n-butanol 13g, Tween 800.3g.
[0039] Preparation:
[0040] (1) Cyhalothrin, spinosad, egg yolk lecithin and Tween 80 are added to soybean oil, mixed evenly, to obtain an oil phase solution;
[0041] (2) under stirring conditions, the above-mentioned oil phase solution is added into water to obtain an oil-water mixture;
[0042] (3) Add n-butanol, matrine and nano-titanium dioxide into water to dissolve, slowly add it dropwise to the above-mentioned oil-water mixture, and control the temperature of the oil-water mixture to be 35°C;
[0043] (4) After the dropwise addition, 300W ultrasonic for 10min, the solution is transparent, and it is ready.
[0044] The average particle diameter of the obtained nanoemulsion insecticide is 70nm.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com