Erasable neutral ink and manufacturing method thereof
A neutral ink, neutral pen technology, applied in ink, home appliances, applications, etc., can solve problems such as poor hand feel, poor writing, blocked pen tips, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0065] The third aspect of the present invention provides a kind of preparation method of erasable neutral ink as described in the present invention, it comprises the steps:
[0066] Provide each component described in the present invention;
[0067] The pigments of the components are dispersed;
[0068] Mix the remaining components evenly to obtain the erasable neutral ink.
[0069] technical effect
[0070] Factors that affect the lubricity of writing include ink viscosity, rheology such as shear thinning, humectants, lubricants, etc. Published patent CN101451037 An erasable neutral ink and its manufacturing method. A moisturizing lubricant is designed in the formula, and ethylene glycol, diethylene glycol, triethylene glycol, glycerin, propylene glycol, polyethylene glycol, polyol and other compositions are selected. . The lubricants described herein are not the above conventional moisturizing lubricants. In order to reduce the frictional resistance during writing, slo...
Embodiment 1
[0087] a) Prepare color paste according to Comparative Example 1. b) 15 grams of deionized water, add 0.8 grams of isomeric alcohol surfactant (XP-90 purchased from BASF, HLB value = 14.5), and add 9.2 grams of oleic acid under stirring to emulsify to a milky white homogeneous liquid; c) Then the remaining 13.3 grams of deionized water, 0.2 grams of anti-corrosion and anti-fungal agent (Proxel XL2, benzotriazole purchased from United Colloids Co., Ltd., the weight ratio of the two is 1:0.5), 2 grams of polycarboxylate Acid sodium salt dispersant (molecular weight 200-2000), 10 grams of ethylene glycol, and 2.0 grams of ammonia water were added to a stirring tank with paddle stirring, and mixed evenly; under stirring, slowly added 2.5 grams of xanthan gum, and the addition was complete After increasing the stirring speed and stirring evenly, finally add the prepared b) and a). Continue to stir and mix evenly, defoaming-filtering-degassing to obtain the product.
Embodiment 2
[0091] a) Prepare color paste according to Comparative Example 1. b) The remaining 28.3 grams of deionized water, 0.2 grams of anti-corrosion and anti-mold agent (Proxel XL2, benzotriazole purchased from United Colloids Co., Ltd., the weight ratio of the two is 1:0.5), 2 grams of poly Carboxylic acid sodium salt dispersant (molecular weight 200-2000), 10 grams of ethylene glycol, 2.0 grams of ammonia water and 10 grams of 2500-mesh talcum powder are added to a stirring tank with paddle stirring, and mixed evenly; under stirring, slowly add After adding 2.5 grams of xanthan gum, increase the stirring speed and stir evenly, then add the prepared pigment slurry at last. Continue to stir and mix evenly, defoaming-filtering-defoaming to obtain the product.
[0092] performance example
[0093](1) The ink sample prepared by the embodiment is equipped with a 640 / 0.4 nib for writing test, and then the sinking amount of the nib ball is measured, so as to analyze the lubricating perfo...
PUM
| Property | Measurement | Unit |
|---|---|---|
| size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 