Integrated terrazzo floor and production method thereof
A manufacturing method and technology for terrazzo, which are applied in building structures, floors, buildings, etc., can solve the problems of short service life of terrazzo, high construction cost, easy cracking and bulging, etc., and achieve low engineering cost, simple construction method, and increased The effect of construction costs
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2015-12-23
- Estimated Expiration
- Not applicable · inactive patent
Abstract
Description
technical field
[0001] The invention belongs to the field of building construction, and in particular relates to an integrated terrazzo floor and a manufacturing method thereof. Background technique
[0002] The floor is a material laid on the ground, which requires a certain strength and rigidity, and has the properties of warmth retention and wear resistance. Concrete has become the building structure material with the largest amount of application and the widest range of use. According to statistics, my country's concrete output in 2012 was as high as 1.2-1.3 billion m3, accounting for about 40% of the world's total output. However, its ubiquitous defects such as easy weathering and cracking, sanding, and non-wear resistance have always been a problem that has plagued people and has attracted widespread attention. Although there are many reasons for this phenomenon, it actually affects and reduces the use effect and life of the terrazzo floor. Contents of the invention...
Examples
Embodiment 1
[0016] (1) After cleaning the surface of the base layer, polish the base layer to make it smooth, not empty, and free of air bubbles;
[0017] (2) Coating release agent on the surface of the base;
[0018] (3) Pour the concrete on the base, smooth it as it pours, and vibrate the grout at the same time until the concrete bleeds evenly;
[0019] (4) 4 hours after concrete pouring, step on the foot and sink 4mm. When the surface is free of bleeding and becomes the initial setting state, the selected Yuhua stone aggregate is evenly sprinkled on the concrete foundation, and then smoothed with a trowel. Wait for complete hydration;
[0020] (5) Use curing wax for curing within 8 hours after the floor is completed, and then polish and polish the floor after 1 week to make the floor show a mirror effect.
[0021] The concrete contains the following raw materials: cement, glass waste, corundum, marble powder, epoxy resin, water; the weight ratio of each raw material is: 35:80:75:50:1...
Embodiment 2
[0024] (1) After cleaning the surface of the base layer, polish the base layer to make it smooth, not empty, and free of air bubbles;
[0025] (2) Coating release agent on the surface of the base;
[0026] (3) Pour the concrete on the base, smooth it as it pours, and vibrate the grout at the same time until the concrete bleeds evenly;
[0027] (4) 3 hours after concrete pouring, step on the subsidence of 5mm, when the surface has no bleeding and is in the initial setting state, the selected Yuhua stone aggregate is evenly sprinkled on the concrete foundation, and then smoothed with a trowel. Wait for complete hydration;
[0028] (5) Use curing wax for curing within 6 hours after the floor is completed, and then polish and polish the floor after 1 week to make the floor show a mirror effect.
[0029] The concrete contains the following raw materials: cement, glass waste, corundum, marble powder, epoxy resin, water; the weight ratio of each raw material is: 35:80:75:50:10:17. ...
Embodiment 3
[0032] (1) After cleaning the surface of the base layer, polish the base layer to make it smooth, not empty, and free of air bubbles;
[0033] (2) Coating release agent on the surface of the base;
[0034] (3) Pour concrete on the base, smooth it as it pours, and vibrate the grout at the same time until the concrete bleeds evenly;
[0035] (4) 5 hours after concrete pouring, step on the subsidence of 5mm, when the surface has no bleeding and is in the initial setting state, the selected Yuhua stone aggregate is evenly sprinkled on the concrete foundation, and then smoothed with a trowel. Wait for complete hydration;
[0036] (5) Use curing wax for maintenance within 12 hours after the floor is completed, and then polish and polish the floor after 1 week to make the floor show a mirror effect.
[0037] The concrete contains the following raw materials: cement, glass waste, corundum, marble powder, epoxy resin, water; the weight ratio of each raw material is: 35:80:75:50:10:17...