Soil improvement method for saline and alkaline land
A technology for soil improvement and saline-alkali land, which is applied in the direction of soil conditioning materials, chemical instruments and methods, applications, etc., can solve problems such as poor water retention effect, poor improvement effect of saline-alkali land, and slowly improve the salinity of saline-alkali land, so as to avoid increase and avoid Salinity and alkalinity, the effect of improving fertilizer efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] A kind of improving agent for improving saline-alkali land, its preparation method is as follows:
[0016] First attapulgite is pulverized to 400 orders for use;
[0017] Then the phosphogypsum is pulverized to 400 mesh for use;
[0018] Add 5 parts by weight of Bacillus subtilis to 60 parts by weight of water, seal and stir, the speed is 2 rpm, the temperature is 30°C, and the time is 6 days; the above is crushed to 400 mesh and 20 parts Parts by weight of attapulgite and 20 parts by weight of phosphogypsum crushed to a fineness of 400 mesh are added to the aforementioned stirred solution, mixed evenly, and left for 3 days; wherein attapulgite can retain nutrients It can be combined with phosphogypsum to increase the air permeability of the soil and avoid soil compaction in saline-alkali land;
[0019] Then add 26 parts by weight of plant ash into the aforementioned mixture, stir evenly, heat to 40°C for 2 days, and cool to room temperature to obtain the modifier, wh...
Embodiment 2
[0022] A kind of improving agent for improving saline-alkali land, its preparation method is as follows:
[0023] At first the attapulgite is pulverized to 450 orders for use;
[0024] Then the phosphogypsum is pulverized to 450 mesh for use;
[0025] Add 8 parts by weight of Bacillus subtilis to 63 parts by weight of water, seal and stir, with a rotating speed of 3 rpm, a temperature of 33°C, and a time of 6 days; crush the aforementioned to 450 mesh and obtain 22 parts Parts by weight of attapulgite and phosphogypsum crushed to a fineness of 450 mesh and 25 parts by weight are added to the aforementioned stirred solution, mixed evenly, and left for 3 days; wherein attapulgite can maintain nutrients It can be combined with phosphogypsum to increase the air permeability of the soil and avoid soil compaction in saline-alkali land;
[0026] Then add 28 parts by weight of plant ash to the aforementioned mixture, stir evenly, heat to 43°C for 2 days, and cool to room temperature...
Embodiment 3
[0029] A kind of improving agent for improving saline-alkali land, its preparation method is as follows:
[0030] First attapulgite is pulverized to 500 orders for use;
[0031] Then the phosphogypsum is pulverized to 500 mesh for use;
[0032] Add 10 parts by weight of Bacillus subtilis to 65 parts by weight of water, seal and stir at a speed of 4 revolutions / s, a temperature of 35°C, and a time of 7 days; crush the aforementioned to 500 mesh and obtain 25 parts Parts by weight of attapulgite and phosphogypsum crushed to a fineness of 500 mesh and 30 parts by weight are added to the aforementioned stirred solution, mixed evenly, and left for 4 days; wherein attapulgite can retain nutrients It can be combined with phosphogypsum to increase the air permeability of the soil and avoid soil compaction in saline-alkali land;
[0033] Then add 30 parts by weight of plant ash into the aforementioned mixed solution, stir evenly, heat to 45° C. for 3 days, and cool to room temperatur...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com