A protective gear and protective gear technology, applied in the field of protective gear materials and its preparation, can solve the problems of wear resistance, general elasticity and toughness, unpleasant smell, and easy breeding of bacteria in functional protective gear, so as to improve the service life and inhibit The effect of the oxidation process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] A sports protective gear material, comprising the following raw materials in parts by weight: 85 parts of polyethylene, 2 parts of nano-radium, 7 parts of tourmaline, 1 part of nano-scale antimony trioxide, 15 parts of chitin, 3 parts of nano-silver, nano-modified 3.5 parts of permanent bamboo charcoal, 2.5 parts of activated carbon, 50 parts of polyvinyl chloride, 6 parts of kaolin, 8 parts of diatomaceous earth, 4 parts of talcum powder, 9 parts of expanded graphite, 0.6 parts of antioxidant, 0.4 parts of light stabilizer, 0.5 parts of heat stabilizer 1.1 parts of plasticizer, 0.7 parts of anti-aging agent and 0.7 parts of compatibilizer.
[0033] Activated carbon is added to the raw material. Activated carbon has a porous structure and can absorb toxic and harmful substances.
[0034] Diatomaceous earth is added to the raw materials. Diatomaceous earth has a natural microporous structure, which can realize breathing and humidity control, and at the same time, it can ...
Embodiment 2
[0047] A sports protective gear material, comprising the following raw materials in parts by weight: 80 parts of polyethylene, 1 part of nano-radium, 5 parts of tourmaline, 0.5 parts of nano-scale antimony trioxide, 10 parts of chitin, 1.5 parts of nano-silver, nano-modified 2.5 parts of permanent bamboo charcoal, 2 parts of activated carbon, 40 parts of polyvinyl chloride, 4 parts of kaolin, 7 parts of diatomaceous earth, 3 parts of talcum powder, 7 parts of expanded graphite, 0.4 parts of antioxidant, 0.2 parts of light stabilizer, and 0.4 parts of heat stabilizer 0.8 parts, 0.8 parts of plasticizer, 0.6 parts of anti-aging agent and 0.5 parts of compatibilizer.
[0048] Activated carbon is added to the raw material. Activated carbon has a porous structure and can absorb toxic and harmful substances.
[0049] Diatomaceous earth is added to the raw materials. Diatomaceous earth has a natural microporous structure, which can realize breathing and humidity control, and at the s...
Embodiment 3
[0062] A sports protective gear material, comprising the following raw materials in parts by weight: 90 parts of polyethylene, 3 parts of nano-radium, 9 parts of tourmaline, 1.5 parts of nano-scale antimony trioxide, 20 parts of chitin, 4.5 parts of nano-silver, nano-modified 4.5 parts of bamboo charcoal, 3 parts of activated carbon, 60 parts of polyvinyl chloride, 8 parts of kaolin, 9 parts of diatomaceous earth, 5 parts of talcum powder, 11 parts of expanded graphite, 0.8 parts of antioxidant, 0.6 parts of light stabilizer, and 0.6 parts of thermal stability 1.4 parts of plasticizer, 0.8 parts of anti-aging agent and 0.9 parts of compatibilizer.
[0063] Activated carbon is added to the raw material. Activated carbon has a porous structure and can absorb toxic and harmful substances.
[0064] Diatomaceous earth is added to the raw materials. Diatomaceous earth has a natural microporous structure, which can realize breathing and humidity control, and at the same time, it can ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com