Embodiment 1
[0045] Embodiment 1, the existing float and its manufacturing method, using high-energy rubber material as the solid core layer 3, carbon fiber material as the core layer 4, and a two-piece cavity mold as examples.
[0046]S1. prepare a two-piece solid core layer cavity mold, the two-piece solid core layer cavity mold is composed of two solid core layer mold plates, and each solid core layer mold plate is evenly arranged with several solid core layers Half cavity, the solid core layer half cavity is to make a solid core layer cavity according to the overall three-dimensional structure of the solid core layer, and then make a thimble cavity through the central axis of the solid core layer cavity, and then mold the solid core layer The cavity is divided into two halves by the longitudinal section of the axis, and the solid core layer half cavity is obtained.
[0047] S2. Make the solid core layer preliminary blank, put the expansion material for making the solid core layer into ...
Embodiment 2
[0055] Embodiment 2, making a two-stage cavity mold.
[0056] The two-stage cavity mold 6 is: the interior of the mold is a cavity, the body structure of the cavity is exactly the same as that of the floating body 1, and the cavity is horizontally divided into two sections from the maximum cross-section of the cavity , that is, the cavity mold is divided into two sections, which become the first section mold 8 and the second section mold 9, forming a two-section cavity mold; one end of the first section mold 8 is called the first top 10, and the first top 10 The center of the thimble is dug with a thimble hole 11, and the diameter of the thimble hole 11 is slightly larger than the diameter of the drift rod 2, that is, the diameter of the thimble hole 11 is 100%-120% of the diameter of the drift rod 2; The other end is called the first clamping end 12; one end of the second segment mold 9 is called the second top 14, and the center of the second top 14 is dug with a thimble hol...
Embodiment 3
[0065] Embodiment 3, the buoy of the present invention and its manufacturing method, use high-energy rubber material as the solid core layer, carbon fiber material as the core layer, and a two-stage cavity mold as an embodiment. This embodiment uses a pen-shaped two-stage type cavity mold.
[0066] In the method for making the buoy of the present invention, firstly, the blank of the solid core layer 3 is made, and then the blank of the core layer 4 is made to make the buoy body 1, and then the buoy rod 2 is inserted, and then the outer layer 5 is made to make the buoy; The solid core layer blank is made by a two-stage solid core layer cavity mold, and the manufacturing steps of the solid core layer blank are as follows.
[0067] S1. A solid core layer 3 blank is produced using a two-stage solid core layer cavity mold.
[0068] S2. Put the expansion material into the mold of the first solid core layer.
[0069] S3. Clamp the second solid core layer mold with the first solid c...