Problems solved by technology

The surfactant in this invention interacts with ingredients such as sodium lauroyl glutamate and cocoyl glycinate, which can promote the foaming of

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Needle-like amino acid crystal cleansing gel and preparation method thereof
  • Needle-like amino acid crystal cleansing gel and preparation method thereof
  • Needle-like amino acid crystal cleansing gel and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

preparation example Construction

[0037]The preparation method of the above-mentioned needle-shaped amino acid crystal cleansing gel comprises the following steps:

[0038] S1. After cleaning and disinfecting the emulsification pot, first add the water in the raw materials of group A to the reaction kettle, then add the remaining raw materials in the raw materials of group A, stir and dissolve completely, the stirring speed is 20-30r / min, and the dissolution temperature is 50 -60°C;

[0039] S2. Heat the solution to 80-85°C, put in the components of phase B in turn, stir and dissolve, put in the raw materials of group C, and keep warm for 30-40min;

[0040] S3. Cool the solution to 70-75°C, dilute the acrylic acid (ester) copolymer in phase D with water in advance, dilute 3-5 times, then slowly put it into the emulsification pot, stir slowly, disperse evenly, and then add pre-dissolved Sodium hydroxide solution in phase E, stir and neutralize for 30min until the material is transparent;

[0041] S4. Cool dow...

Embodiment 1

[0045] A needle-shaped amino acid crystal cleansing gel, including the following components:

[0046] Phase A components: 15 parts of water, 0.15 parts of disodium EDTA, 14 parts of glycerin;

[0047] Phase B components: 12 parts of cocamidopropyl betaine, 10 parts of potassium cocoyl glycinate, 2 parts of disodium lauryl sulfosuccinate, 1 part of decyl glucoside, 1 part of glyceryl oleate, formazan 10 parts of sodium cocoyl taurate, 0.2 parts of quaternary ammonium salt-80, 0.3 parts of sodium isostearyl lactylate, 0.15 parts of plant amino acids, 0.15 parts of methylparaben, N-lauroyl-N-methyl 0.6 part of sodium taurate, 0.3 part of dodecyltrimethylammonium chloride, and 0.3 part of dodecyldimethyl betaine.

[0048] Phase C components: 12 parts of taurine.

[0049] Phase D components: 8 parts of acrylic (ester) copolymer, 17 parts of water.

[0050] Phase E components: 0.065 parts of sodium hydroxide.

[0051] Phase F components: 0.5 parts of phenoxyethanol, 0.0005 parts...

Embodiment 2

[0060] A needle-shaped amino acid crystal cleansing gel, including the following components:

[0061] Phase A components: 16 parts of water, 0.1 part of disodium EDTA, 17 parts of glycerin;

[0062] Phase B components: 10 parts of cocamidopropyl betaine, 12 parts of potassium cocoyl glycinate, 1 part of disodium lauryl sulfosuccinate, 1.2 parts of decyl glucoside, 1.5 parts of glyceryl oleate, formazan 11 parts of Sodium Cocoyl Taurate, 0.2 parts of Quaternary Ammonium Salt-800, 0.2 parts of Sodium Isostearyl Lactyl Lactylate, 0.1 part of Vegetable Amino Acids, 0.2 parts of Methylparaben, N-Lauroyl-N-Methyl 0.6 parts of sodium taurine, 0.3 parts of dodecyltrimethylammonium chloride, and 0.3 parts of dodecyldimethyl betaine.

[0063] Phase C components: 14 parts of taurine.

[0064] Phase D components: 9 parts of acrylic (ester) copolymer, 12 parts of water.

[0065] Phase E components: 0.069 parts of sodium hydroxide.

[0066] Phase F components: 0.4 parts of phenoxyethano...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses needle-like amino acid crystal cleansing gel and a preparation method thereof, and belongs to the field of daily chemical products. The cleansing gel is prepared from the following components: a phase A component comprising water, EDTA disodium and glycerol; and a phase B component comprising cocamidopropyl betaine, potassium cocoyl glycinate, disodium lauryl sulfosuccinate, decyl glucoside, glyceryl oleate, sodium methyl cocoyl taurate, quaternary ammonium salt-80, sodium isostearoyl lactylate, plant amino acids, methylparaben, N-lauroyl-N-sodium methyl taurate, dodecyl trimethyl ammonium chloride and dodecyl dimethyl betaine. Electrostatic attraction exists between the N-lauroyl-N-sodium methyl taurate and the dodecyl trimethyl ammonium chloride and the dodecyl dimethyl betaine, so that the effect of synergistically improving the foam stability is achieved.

Description

technical field [0001] The invention belongs to the field of daily chemical products, and in particular relates to a needle-like amino acid crystal cleansing gel and a preparation method thereof. Background technique [0002] Cleansing creams on the market can be roughly divided into soap-based systems, surfactant systems, emulsifying systems, amino acid systems, etc. Soap-based cleansing cream has excellent foaming power and cleaning power, and the skin feels refreshing when washed. However, it is alkaline and has strong degreasing power. It will feel tight after washing. Long-term use will cause greater irritation and damage to the skin. Compared with the soap-based system, the surfactant system is less irritating and has moderate degreasing power, but the surfactant is easy to remain, it is not easy to be cleaned, and there is a slippery feeling after washing. The emulsified system cleanser feels moisturizing after washing, but the cleaning power is slightly weaker, and ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): A61K8/41A61K8/44A61K8/46A61K8/02A61Q19/10
CPCA61K8/442A61K8/416A61K8/44A61K8/466A61K8/0291A61Q19/10A61K2800/5922
Inventor 李继德吴华养李空军陈思钰
Owner 美丽链接生物科技研究院(广东)有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products