A low-temperature co-fired ceramic and common-mode filter technology, applied in waveguide-type devices, inductors, fixed inductors, etc., can solve problems such as poor impedance characteristics, failure to filter noise, and inability to effectively reduce differential mode impedance. Achieve the effect of reducing line spacing requirements, low processing difficulty, and reducing electromagnetic leakage
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2007-09-19
Smart Images
Figure 1 Figure 2 Figure 3
Abstract
Description
technical field
[0001] The invention relates to a low-temperature co-fired ceramic common-mode filter for eliminating signal interference of electronic equipment. technical background
[0002] There are currently two main types of chip common mode filters, which are multi-layer chip and wire-wound. The wire-wound filter has better electrical performance, but the cost is high, and it is not suitable for large-scale use in electronic products. . One of the multi-layer chips is a double-layer coupled ferrite structure. Due to the characteristics of the ferrite material itself, the loss in the high-frequency band is too large. When the device is used in the high-frequency band, the useful differential The mode signal causes great attenuation, which affects the circuit performance, so it is only suitable for lower frequency bands; on the other hand, the dielectric constant of the ferrite material is relatively high. In order to meet the characteristic impedance requirements of t...
Examples
Embodiment Construction
[0029] As shown in Figure 2 and Figure 3, the chip type low temperature co-fired ceramic common mode filter (n is 7 in this example, the printing of each layer is shown in Figure 4-1, Figure 4-2, Figure 4-3, Figure 4 -4, shown in Fig. 4-5, Fig. 4-6), it is made of low-temperature co-fired ceramic body 1 by stacking tape-cast green tapes, and there are 7 layers of left and right layers printed on the low-temperature co-fired ceramic body. Coil and right coil, the 7th layer and the 1st layer are pin layers respectively; one end of the left coil 4 on the 7th layer is connected to one end of the right coil 9 on the 6th layer by a joint 8 (Note: in Figure 2, outside the figure The joint is one end, the joint in the picture is the other end, and the pin is the outer end), the other end of the right coil 9 on the 6th layer is connected with the other end of the left coil on the 5th layer by a joint; the right coil on the 7th layer The other end of 7 is connected with the other end of...