Compound material constructed by molecular engram and fluorescent conjugated polymer, preparation and application
A technology of conjugated polymers and molecular imprinting, which is applied in the direction of material inspection products, fluorescence/phosphorescence, material excitation analysis, etc., and can solve the problems of unsuitable for on-site, fast, sensitive and highly selective detection, slow response, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] Embodiment 1 synthesis process is as follows:
[0034] Side chain (12 carbons) TNT-sensitive fluorescent conjugated polymer containing molecularly imprinted active monomer 1mmol (see Figure 4 for the structure), acrylamide (1mmol), di(methacrylate)-ethylene glycol ester (4mmol) , explosive template molecule (containing Octogen, RDX, nitroglycerin, the ratio of the three is 1:1:1, 0.018mmol in total), add 0.012mmol of benzoyl peroxide, dissolve in 5mL of toluene, and heat to React at 60-70°C for 6 hours. The resulting polymer was precipitated, centrifuged, and the polymer was washed successively with toluene and ethanol. Soxhlet extractor extracts and removes template molecules to obtain a light yellow composite polymer with a yield of 85%.
Embodiment 2
[0035] Embodiment 2 (change crosslinking monomer), synthetic process is as follows:
[0036] Double side chain (12 carbons) TNT-sensitive fluorescent conjugated polymer containing molecularly imprinted active monomer 1mmol (see Figure 4 for the structure), acrylic acid (1mmol), di(methacrylic acid)-ethylene glycol ester (4mmol) , explosive template molecule (containing Octogen, RDX, nitroglycerin, the ratio of the three is 1:1:1, 0.018mmol in total), add 0.012mmol of benzoyl peroxide, dissolve in 5mL of toluene, and heat to React at 60-70°C for 6 hours. The resulting polymer was precipitated, centrifuged, and the polymer was washed successively with toluene and ethanol. Soxhlet extractor extracts and removes template molecules to obtain a light yellow composite polymer with a yield of 87%.
Embodiment 3
[0037] Embodiment 3 (carbon chain length changes)
[0038] Double side chain (6 carbons) TNT-sensitive fluorescent conjugated polymer containing molecularly imprinted active monomer 1mmol (see Figure 4 for structure), acrylamide (1mmol), di(methacrylic acid)-ethylene glycol ester (4mmol ), explosive template molecules (containing Octogen, RDX, and nitroglycerin, the ratio of which is 1:1:1, 0.018mmol in total), add 0.012mmol of benzoyl peroxide, dissolve in 5mL of toluene, and heat Reaction at 60-70°C for 6 hours. The resulting polymer was precipitated, centrifuged, and the polymer was washed successively with toluene and ethanol. Soxhlet extractor extracts and removes template molecules to obtain a light yellow composite polymer with a yield of 90%. The product is less soluble in common solvents such as DMF and DMSO. Not suitable for further device preparation.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 