Manufacturing method of hollow fiber membrane component
A manufacturing method and fiber membrane technology, applied in the field of membrane separation, can solve the problem that the single-ended hole blocking membrane wire cannot be freely swayed, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0013] Such as figure 1 Shown, a kind of manufacturing method of hollow fiber membrane module is carried out according to the following steps: (1) cast one end of several hollow fiber membranes with the same length according to a known method and hollow fiber membranes are perforated, and all hollow fiber membranes Cut the second ends of the filaments to the required length; (2) place molten hot melt adhesive with a softening point of about 62°C in the container 5 and keep it warm; extend the second ends of all hollow fiber membranes into the hot melt adhesive in the container 5mm in the center, stay for 2min; after tightening the end cap 4, connect the vacuum pump 1 to vacuumize, and connect the precision vacuum gauge 2 in the middle; (3) turn off the vacuum pump and keep the pressure at -0.002Mpa; cool down until the hot melt glue solidifies; (4) then Cut off the bottom 10mm of the second end of all the hollow fiber membranes; the effect that the holes of the hollow fiber me...
Embodiment 2
[0015] Such as figure 1 Shown, a kind of manufacturing method of hollow fiber membrane module is carried out according to the following steps: (1) cast one end of several hollow fiber membranes with the same length according to a known method and hollow fiber membranes are perforated, and all hollow fiber membranes Cut the second end of the wire to the required length; (2) place the prepared epoxy resin in the container 5, extend the second end of all the hollow fiber membrane wires into the epoxy resin for 10 mm, and stay for 1 min; put the end cap 4 After tightening, connect with vacuum pump 1 for vacuuming, and connect precision vacuum gauge 2 in the middle; (3) Turn off the vacuum pump and keep the pressure at -0.001Mpa until the epoxy resin is cured; (4) Then cut off the second end of all hollow fiber membranes If the bottom is 20 mm, the hollow fiber membrane pores are completely blocked but the hollow fiber membranes are dispersed.