Compound agent for repairing heavy metal contaminated soil and application thereof
A technology of polluted soil and heavy metals, applied in the direction of restoration of polluted soil, application, soil conditioning materials, etc., can solve the problem of low stability rate of heavy metals, achieve the effect of improving stability efficiency and alleviating the leaching of cadmium
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Example Embodiment
[0034] Example 1:
[0035] Test sample and restoration goal: Collect a portion of the lower clayey soil at a pesticide factory in Hunan, and pass it through a 2mm sieve after natural air drying. The total arsenic and cadmium content of the soil are 1729mg / kg and 11mg / kg, respectively. The arsenic and cadmium concentrations of the extract are respectively. It was 6.80 and 0.012mg / L, and the pH was 8.11 (Table 1). The soil leaching method is in accordance with the HJ / T 557-2009 standard of "Solid waste leaching toxicity leaching method horizontal oscillation method". After restoration, the soil leaching solution must meet the requirements of the "Surface Water Environmental Quality Standard" GB 3838-2002 IV standard (Cd <5μg / L; As <50μg / L). The compliance and stability efficiency requirements of arsenic and cadmium are 99.3% and 58% respectively.
[0036] Pharmaceutical preparation: Weigh 50g of iron sulfate, 20g of ferrous sulfate, 20g of calcium carbonate, 9g of sodium lignosulfon...
Example Embodiment
[0041] Example 2:
[0042] Test samples and restoration targets: Collect surface sandy soil in a project in Baiyin, Gansu, and pass through a 2mm sieve after natural air drying. The total arsenic and cadmium contents are 153.8 and 23.8 mg / kg, respectively, and the arsenic and Cd concentrations in the leachate are 77 and 45 μg / g, respectively. L, pH is 6.93 (Table 2). The soil leaching method is in accordance with the HJ / T 557-2009 standard of "Solid waste leaching toxicity leaching method horizontal oscillation method", and the soil leaching solution after restoration must meet the requirements of "Groundwater Environmental Quality Standard" (GB / T 14848-2017) III standard (Cd) <10μg / L; Arsenic <50μg / L). The compliance and stability efficiency requirements of arsenic and cadmium are 35% and 77.8% respectively.
[0043] Pharmaceutical preparation: Weigh 43g of iron sulfate, 28g of calcium hydroxide, 20g of heavy calcium carbonate, 6g of sodium lignosulfonate and 3g of dehydrated thi...
Example Embodiment
[0048] Example 3:
[0049] Test sample and restoration target: Collect surface miscellaneous fill in a chemical plant in Hunan, and pass it through a 2mm sieve after natural air drying. The total arsenic (As), cadmium (Cd), lead (Pb) and zinc (Zn) contents are 1359 respectively , 509, 13399 and 20100 mg / kg, the concentration of As, Cd, Pb and Zn in the extract were 277, 468, 279 and 1820 μg / L, respectively, and the pH was 7.14 (Table 6). The soil leaching method complies with the HJ / T 557-2009 standard of "Solid waste leaching toxicity leaching method horizontal oscillation method", and the soil leaching solution after restoration shall meet the requirements of the "Surface Water Environmental Quality Standard" GB 3838-2002 IV standard. As, Cd, Pb and Zn meet the standard and stable efficiency requirements of 81.9%, 98.9%, 82.1% and 45% respectively.
[0050] Pharmaceutical preparation: weigh 35g of iron sulfate, 10g of calcium hydroxide, 40g of heavy calcium carbonate, 5g of sodi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap