A technology of soil remediation agent and high-alumina bauxite, which is applied in the field of environmental governance, can solve the problems of reducing the repair cycle and failing to guarantee the repair effect, and achieve the effect of reducing the repair cycle, good repair effect and reducing migration
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] A soil restoration agent, comprising the following raw materials: 40 kilograms of phosphogypsum, 15 kilograms of caustic soda, 32 kilograms of basic slag, 6 kilograms of calcium-based bentonite, 4 kilograms of high alumina bauxite, 8 kilograms of white boronite, modified vermiculite 80 kg, and the right amount of water. Wherein, the modified vermiculite is prepared by crushing the vermiculite, filling it with liquid nitrogen and drying it, then mixing it with polypropylene glycol, butyl titanate and sulfuric acid (concentrated sulfuric acid with a concentration of 98wt%), and then calcining. have to. Specifically, the preparation method of the modified vermiculite is: according to the mass ratio of vermiculite, polypropylene glycol, butyl titanate and sulfuric acid of 9:7:0.5:0.5, respectively weigh vermiculite, polypropylene glycol, titanium Butyl acid and sulfuric acid, crush the weighed vermiculite to 100 mesh, add water for ultrasonic treatment (ultrasonic frequenc...
Embodiment 2
[0035]A soil remediation agent, including the following raw materials: 80 kg of phosphogypsum, 40 kg of caustic soda, 48 kg of alkaline slag, 20 kg of calcium-based bentonite, 10 kg of high alumina bauxite, 18 kg of white boronite, modified vermiculite 160 kg, and the right amount of water. Wherein, the modified vermiculite is prepared by crushing the vermiculite, filling it with liquid nitrogen and drying it, then mixing it with polypropylene glycol, butyl titanate and sulfuric acid (concentrated sulfuric acid with a concentration of 98wt%), and then calcining. have to. Specifically, the preparation method of the modified vermiculite is: according to the mass ratio of vermiculite, polypropylene glycol, butyl titanate and sulfuric acid to 20:10:2:2, respectively weigh vermiculite, polypropylene glycol, titanium Butyl acid and sulfuric acid, crush the weighed vermiculite to 400 mesh, add water to carry out ultrasonic treatment (ultrasonic frequency is 60kHz, ultrasonic power i...
Embodiment 3
[0041] A soil remediation agent, including the following raw materials: 56 kg of phosphogypsum, 18 kg of caustic soda, 38 kg of basic slag, 8 kg of calcium-based bentonite, 6 kg of high alumina bauxite, 10 kg of white boronite, modified vermiculite 100 kg, and the right amount of water. Wherein, the modified vermiculite is prepared by crushing the vermiculite, filling it with liquid nitrogen and drying it, then mixing it with polypropylene glycol, butyl titanate and sulfuric acid (concentrated sulfuric acid with a concentration of 98wt%), and then calcining. have to. Specifically, the preparation method of the modified vermiculite is: according to the mass ratio of vermiculite, polypropylene glycol, butyl titanate and sulfuric acid to 12:8:0.9:0.9, respectively weigh vermiculite, polypropylene glycol, titanium Butyl acid and sulfuric acid, crush the weighed vermiculite to 200 mesh, add water for ultrasonic treatment (ultrasonic frequency is 40kHz, ultrasonic power is 30W) and...