Flotation collector for scheelite
A collector and scheelite technology, applied in the field of mineral flotation collectors and flotation collectors, can solve the problems of high production cost, limited widespread popularization and application, etc., and achieve low cost, increased dispersion performance, and effective Good results
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The scheelite flotation collector of this embodiment is prepared from the following raw materials in weight percentage: 20% of tetrasodium sulfosuccinic acid, 25% of iquipon T, 15% of isooctyl phosphate, fatty acid Sodium 40%, weigh the raw materials respectively according to the above weight percentage, heat fatty acid sodium to 60°C-70°C, add tetrasodium sulfosuccinic acid and stir, then add iquipon T and isooctyl phosphate Stir for 1.5 hours, and stir evenly to prepare a scheelite flotation collector.
[0026] Using the prepared scheelite flotation collector, the flotation grade of raw ore is 0.45%, and the obtained tungsten crude concentrate grade reaches 1.25%, and the recovery rate is a good indicator of 88.17%.
Embodiment 2
[0028] The scheelite flotation collector of this embodiment is prepared from the following raw materials in weight percentage: 21% of tetrasodium sulfosuccinic acid, 26% of Iquipon T, 14% of isooctyl phosphate, fatty acid Sodium 39%, weigh the raw materials respectively according to the above weight percentage, heat fatty acid sodium to 60°C-70°C, add tetrasodium sulfosuccinic acid and stir, then add iquipon T and isooctyl phosphate Stir for 1.5 hours, and stir evenly to prepare a scheelite flotation collector.
[0029] Using the prepared scheelite flotation collector, the flotation grade of raw ore is 0.45%, and the obtained tungsten crude concentrate grade reaches 1.26%, and the recovery rate is a good indicator of 87.62%.
Embodiment 3
[0031] The scheelite flotation collector of this embodiment is prepared from the following raw materials in weight percentage: 22% of tetrasodium sulfosuccinic acid, 27% of iquipon T, 13% of isooctyl phosphate, fatty acid Sodium 38%, weigh the raw materials respectively according to the above weight percentage, heat fatty acid sodium to 60°C-70°C, add tetrasodium sulfosuccinic acid and stir, then add iquipon T and isooctyl phosphate Stir for 1.5 hours, and stir evenly to prepare a scheelite flotation collector.
[0032] Using the prepared scheelite flotation collector, the flotation grade of raw ore is 0.45%, and the obtained tungsten crude concentrate grade reaches 1.25%, and the recovery rate is a good indicator of 87.85%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com