A detection method and uniformity technology, applied in chemical instruments and methods, measuring devices, and disease resistance to media transmission, etc., can solve problems such as time-consuming and labor-intensive inconvenient, achieve simple methods, improve fluorescence quantum yield, and experiment The effect is simple and convenient
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0058] The present embodiment provides a kind of coating method of 7-hydroxy bismethyl percarbon spiro coumarin, and the method comprises the following steps:
[0059] 2.0 mmol of 7-hydroxybismethyl all-carbon spiro coumarin compound, 30 mL of methanol and 1.0 mmol of MOF-808 were added to the reaction flask in sequence, and after stirring at room temperature for 3.0 h, suction filtration was performed with a filter funnel, and air was allowed to dry naturally. After drying, the coated product MOF-808@coumarin can be obtained.
[0060] In this example, the simulation simulation of the coating product MOF-808@coumarin was carried out, and its coating form was 1-7(7-hydroxybismethyl percarbon spirocoumarin)@MOF-808, and the coating simulation structure such as figure 1 shown.
[0061] from figure 2 It can be seen that the 7-hydroxybismethyl percarbon spirocoumarin in this example is obviously coated by MOF-808, and the coated product MOF-808@coumarin is obtained.
[0062] f...
Embodiment 2
[0073] This embodiment provides a coating method of CL-20, such as Figure 4 As shown, the method includes the following steps:
[0074] Step 1, 7-hydroxybismethyl all-carbon spiro coumarin coating:
[0075] Adopt the coating method of 7-hydroxybismethyl percarbon spirocoumarin in Example 1.
[0076] Step 2, CL-20 coating:
[0077] Add 0.1 mmol melamine formaldehyde resin prepolymer to the reaction flask and dissolve it in 40 mL of toluene, then add 2.0 mmol CL-20, 1.0 mmol MOF-808@coumarin, mix evenly, add 3 drops of citric acid catalyst, and ultrasonically disperse evenly , the temperature was raised to 40° C. and stirred for 3.0 h to carry out in-situ polymerization (the process of coating reaction can also be detected by an ultraviolet lamp with a wavelength of 365 nm). After the coating is completed, suction filtration with a filter funnel, and air-dry to obtain a CL-20 coating product, such as Figure 5 shown.
[0078] Sensitivity test: Comparing the sensitivity of ...
Embodiment 3
[0080] The present embodiment provides an intuitive detection method for the coating uniformity of CL-20, which comprises the following steps:
[0081] Step 1, 7-hydroxybismethyl all-carbon spiro coumarin coating:
[0082] Adopt the coating method of 7-hydroxy bismethyl percarbon spiro coumarin in step 1 of embodiment 2.
[0083] Step 2, CL-20 coating:
[0084] Coating with CL-20 in step 2 of Example 2.
[0085] Step three, intuitive detection:
[0086] The coating product obtained in the second step is directly irradiated with an ultraviolet lamp with a wavelength of 365 nm, and the uniformity of the coating product can be visually detected through the solid-state fluorescence distribution.
[0087] The results of the intuitive detection are:
[0088] First, when the uniform fluorescence distribution area on the coating product is equal to 100%, the coating uniformity is good; (visual inspection: the coating product is irradiated under a 365nm ultraviolet lamp, and the fl...
PUM
Property | Measurement | Unit |
---|---|---|
wavelength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com