Fast quartz and feldspar identifying method
A technology of quartz and feldspar, applied in the direction of solid separation, measuring devices, instruments, etc., can solve difficult problems and achieve the effect of simple equipment, convenient operation and easy method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0006] First, put the monomer particle size quartz and feldspar to be identified into an acid-resistant container; secondly, add hydrofluoric acid with a volume concentration ratio of 30-60% in the container to cover all the samples, and stir while adding; The third is that the soaking time of the sample is 5-300 seconds; the fourth is to pour out the hydrofluoric acid, rinse the sample with water and then dry it. Observing under binoculars, it can be found that the mineral with smooth, clean and basically transparent surface is quartz; while the mineral with rough surface, powder shape, translucent or opaque is feldspar. According to these phenomena, quartz and feldspar can be identified.
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com