Comprehensive utilization method for red mud

A red mud and compound technology, which is applied in the preparation of alkaline earth metal aluminate/alumina/hydroxide, etc., can solve the problems of difficulty in realizing the comprehensive utilization of red mud, insufficient utilization, low utilization rate, etc., and achieve utilization High efficiency, high added value, and wide application range

Inactive Publication Date: 2008-10-01
WUHAN UNIV OF SCI & TECH
View PDF0 Cites 31 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] Research on the use of red mud to produce cement (Ren Dongmei, Mao Yanan. Comprehensive utilization of red mud [J]. Nonferrous Metal Industry, 2002, [5]: 57-58), due to the high alkali content of red mud, the ratio of red mud is affected by cement The restriction of alkali content limits the application of red mud as a raw material for cement production. The comprehensive utilization rate of red mud is only 35% to 50%, and the utilization rate is low.
[0005] Charcoal reduction of iron in red mud, the method of recovery by magnetic separation process (Liao Chunfa, Jiang Guoping. Technology research on iron recovery from red mud. China Mining. Volume 16 No. 2. February 2007), but due to A large amount of SiO in red mud 2 , Al 2 o 3 , CaO and other substances are not fully utilized, and the cost is high, the utilization rate is low, and it is difficult to realize the comprehensive utilization of red mud

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0013] A method for comprehensive utilization of red mud. First, mix 9-11wt% coke and red mud with the red mud and place it in an electric arc furnace. Melt the mixture at 1400-1500°C and keep it warm for 0.5-1 hour. The upper layer is made of calcium aluminate material, and the lower layer is made of silicon. Ferroalloy; then after natural cooling, it is crushed and separated to obtain calcium aluminate and ferrosilicon alloy blocks. The main phase of the obtained calcium aluminate material is CA 2 and CA 6 .

[0014] The red mud in this example is Bayer process red mud, and its main chemical composition is: SiO 2 18-20wt%, Fe 2 o 3 35~40wt%, Al 2 o 3 18~20wt%, CaO 3~4wt%, MgO 0.5~1wt%, K 2 O is 0.1~0.3wt%, Na 2 O is 6~11wt%, TiO 2 1.5-2wt%, ignition loss 9-12wt%.

Embodiment 2

[0016] A method for comprehensive utilization of red mud. First mix 7-10% of the mass of red mud with coke and 4-6% of the mass of red mud with limestone and put it in an electric arc furnace. The CaO in the limestone is 53.34wt%; The mixture is melted and kept warm for 1-1.5 hours, the upper layer is calcium aluminate material, and the lower layer is ferrosilicon alloy; finally, after natural cooling, it is broken and separated to obtain calcium aluminate and ferrosilicon alloy blocks. The main phase of the obtained calcium aluminate material is CA 2 .

[0017] The red mud composition in this example is Bayer process red mud, and its main chemical composition is: SiO 2 10~15wt%, Fe 2 o 3 30~36%wt, Al 2 o 3 15-20wt%, CaO 3-10wt%, MgO 0.5-1wt%, K 2 O is 0.1~0.3wt%, Na 2 O is 6~10wt%, TiO 2 1.5-2wt%, ignition loss 9-12wt%.

Embodiment 3

[0019] A method for comprehensive utilization of red mud. 7-11wt% anthracite of red mud mass and 6-14wt% limestone of red mud mass are firstly mixed with red mud and placed in electric arc furnace, and CaO in limestone is 53.34%. Then the mixture is fused and reduced at 1500-1550°C, and kept for 1-1.5 hours. The upper layer is calcium aluminate material, and the lower layer is ferrosilicon alloy; finally, after natural cooling, it is broken and separated to obtain calcium aluminate and ferrosilicon alloy blocks. The main phase of the obtained calcium aluminate material is CA 2 and CA.

[0020] The red mud composition in this example is Bayer process red mud, and its main chemical composition is: SiO 2 11~15wt%, Fe 2 o 3 35~38%wt, Al 2 o 3 18~20wt%, CaO 3~4wt%, MgO 1~2wt%, K 2 O is 0.1~0.3wt%, Na 2 O is 6~11wt%, TiO 2 1.5-2wt%, ignition loss 9-12wt%.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention belongs to the technical field of comprehensive utilization of red mud. The technical proposal of the invention is that: adding coke, anthracite which is 7-75% of mass of red mud, calcium compound which is 0-16% or aluminiferous compounds which is 0-645% into the red mud, placing in an electrical furnace after mixing; melting to deoxidize at the temperature ranging from 1400 to 1800 DEG C, and keeping temperature for 0.5 to 4 hours, crushing the red mud for separation after naturally cooling. The main chemical ingredients of the red mud is that: SiO<2> is 10-23wt%, Fe<2>O<3> is 7-40wt%, Al<2>O<3> is 6-20wt%, CaO is 3-45 wt%, Mgo is 0.5-3 wt%, K<2>O is 0.1-0.4 wt%, Na<2>O is 2-11 wt%, TiO<2> is 1-6 wt%, cauterized loss is 8-12wt%. Under high temperature, SiO<2> and Fe<2>O<3> in the red mud of the invention are deoxidized into ferro-silicon alloy, Al<2>O<3> and CaO are generated to calcium aluminate, Na<2>O and K<2>O are volatilized at high temperature to be refined, cooled and deposited to obtain the calcium aluminate material and ferro-silicon alloy by crushing separation, so the invention has the characteristics of wide application range and high additional value.

Description

technical field [0001] The invention belongs to the technical field of comprehensive utilization of red mud. In particular, it relates to a method for preparing ferrosilicon alloy and calcium aluminate material by using electric smelting reduction red mud. Background technique [0002] Red mud is solid powdery waste discharged during the production process of alumina smelting industry. Generally, about 1.0-1.7 tons of red mud are produced for every ton of alumina produced. According to incomplete estimates, the world discharges about 60 million tons of red mud every year. my country is the world's fourth largest producer of alumina, and its accumulated red mud stockpile has reached 41 million tons. A large amount of red mud is stored in the open air, occupying farmland and hills, and the dust is flying, causing environmental and air pollution. The pH of red mud is very high, and its leachate is about 12.1 to 13.0. The lye in the red mud seeps into the formation with the r...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C22B5/02C22B5/04C22B5/10C22C38/02C01F7/16
Inventor 李远兵胡建宝黄凯李亚伟赵雷祝泉金胜利李淑静雷中兴
Owner WUHAN UNIV OF SCI & TECH
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products