A patch and plasticizer technology, applied in the direction of non-active ingredient medical preparations, medical preparations containing active ingredients, sheet-like delivery, etc., can solve complex production process, skin damage, low drug transdermal rate, etc. problems, achieve excellent safety and less skin irritation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] Prescription (based on 1000 stickers): tulobuterol 1.0g, polyethylene glycol 400 2.8g, oleic acid 0.2g, acrylic pressure-sensitive adhesive 36g.
[0019] Process: Dissolve the drug in an appropriate amount of ethanol, add polyethylene glycol 400, oleic acid and acrylic pressure-sensitive adhesive, mix well, coat on the anti-adhesive layer, dry at 60°C, cover the backing layer, punch Cut into 22.4mm×22.4mm, obtain the tulobuterol patch containing 2.5% mass tulobuterol and 0.5% mass oleic acid in the adhesive layer.
Embodiment 2
[0021] Prescription (based on 1000 stickers): tulobuterol 1.0g, polyethylene glycol 400 2.8g, isopropyl myristate 4g, acrylic pressure-sensitive adhesive 32.2g.
[0022] Process: Dissolve the drug in an appropriate amount of ethanol, add polyethylene glycol 400, isopropyl myristate and acrylic pressure-sensitive adhesive, mix well, apply on the release layer, dry at 60°C, and cover the upper back The liner was punched and cut into 22.4mm×22.4mm to obtain a tulobuterol patch containing 2.5% by mass tulobuterol and 10% by mass isopropyl myristate in the adhesive layer.
Embodiment 3
[0024] Prescription (based on 1000 stickers): tulobuterol 1.0g, polyethylene glycol 400 2.8g, polyacrylic resin 4g, acrylic pressure-sensitive adhesive 32.2g.
[0025] Process: Dissolve the drug and polyacrylic acid resin in an appropriate amount of ethanol, add polyethylene glycol 400 and acrylic pressure-sensitive adhesive, mix well, coat on the anti-adhesive layer, dry at 60°C, cover the backing layer, Die into 22.4mm * 22.4mm, obtain the tulobuterol patch that contains 2.5% mass tulobuterol and 10% mass polyacrylic acid resin in the adhesive layer.
PUM
Property | Measurement | Unit |
---|---|---|
Peel strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com