Preparation process for rapidly-dissolving granular sodium percarbonate
A technology for sodium percarbonate and preparation process, applied in the field of inorganic salts, can solve problems such as being difficult to meet the requirements of sodium percarbonate, and achieve the effects of being environmentally friendly, reducing production costs, and having small investment in equipment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Add 5kg of light soda ash to a 20L double cone mixer, add 19.1g of solid stabilizer magnesium sulfate at the same time, weigh 4.38kg of hydrogen peroxide solution (in the form of H 2 o 2 50.1% in total), and add 0.1kg of diethylenetriaminepentamethylenephosphonic acid (DTPMP) and its sodium salt solution, stir and mix evenly. Spray the prepared hydrogen peroxide solution into the double cone mixer, turn on the refrigerated circulating water to cool down, when the hydrogen peroxide spray reaches 3.5kg, the water content of the system is 20.9%, stop spraying the hydrogen peroxide solution, and stir for 2 minutes to complete the reaction. Add 1.7kg of granulated Yuanming powder, and the sodium percarbonate powder instantly becomes expanded wet granules of sodium percarbonate. Dry in a small fluidized bed to obtain dry fast-dissolving sodium percarbonate granules with 10% active oxygen, 1.5% moisture, 0.15-1.2mm particle size, and a T90 (20°C) of 18s.
Embodiment 2
[0019] Add 6kg of light soda ash to a 20L double cone mixer, add 44.7g of solid stabilizer sodium metasilicate at the same time, weigh 4.2kg of hydrogen peroxide solution (in the form of H 2 o 2 60.2% in total), and add 0.08kg of diethylenetriaminepentamethylenephosphonic acid (DTPMP) and its sodium salt solution, stir and mix evenly. Spray the prepared hydrogen peroxide solution into the double cone mixer, turn on the refrigerated circulating water to cool down, when the hydrogen peroxide spray reaches 3.34kg, the water content of the system is 15.6%, stop spraying the hydrogen peroxide solution, and stir for 2 minutes to complete the reaction. Add 1.54kg of granulated sodium sulfate and 0.4kg of light soda ash granules, and the sodium percarbonate powder instantly becomes puffed wet granules of sodium percarbonate, dried in a small fluidized bed to obtain fast-dissolving sodium percarbonate with 11.2% active oxygen Dry granules, moisture 1.2%, particle size 0.15-1.2mm, T90 ...
Embodiment 3
[0021] Add 10kg of light soda ash to a 20L double cone mixer, add 142g of solid stabilizer sodium tripolyphosphate at the same time, weigh 8.75kg of hydrogen peroxide solution (in H 2 o 2 50.1% in total), and add 0.9kg of diethylenetriaminepentamethylenephosphonic acid (DTPMP) and its sodium salt solution, stir and mix evenly. Spray the prepared hydrogen peroxide solution into the double-cone mixer, turn on the refrigerated circulating water to cool down, when the hydrogen peroxide is sprayed to 7kg (the water content in the system is 21.9%), stop spraying the hydrogen peroxide solution, and stir for 2 minutes to complete the reaction. Add 2.1 kg light soda ash granules and 28g sodium carboxymethyl cellulose (CMC), stirred for 3 minutes, the sodium percarbonate powder instantly becomes expanded sodium percarbonate wet granules. Small-scale fluidized bed drying, to obtain 12.0% active oxygen fast Dissolved sodium percarbonate dry product, moisture 0.8%, particle size 0.15-...
PUM