Preparation method of plant-embedded resin craftwork
A technology of handicrafts and plants, applied in the production of resin handicrafts, can solve the problems of poor viewing, affecting viewing, dehydration deformation, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Select a peach blossom with beautiful shape and complete appearance, bury it in aluminum hydroxide powder (Sinopharm Group, CP grade), take it out after 24 hours, carefully remove the aluminum hydroxide powder on the surface of the peach blossom with a small brush, and glue the peach blossom with 502 glue Fix it in the center of the bottom of the mold, add 5 / 1000 volume of accelerator to 1 volume of unsaturated polyurethane resin, and then add 8 / 1000 volume of curing agent, stir evenly and naturally cool down to 30°C and pour it into the mold , take it out after solidification.
Embodiment 2
[0021] Select a peach blossom with a stem of about 3 cm, bury it in calcium chloride powder (Sinopharm Group, CP grade), take it out after 12 hours, carefully remove the calcium chloride powder on the surface of the peach blossom with a small brush, and insert a Use iron wire of suitable size to increase the strength of the flower stem. Fix the peach flower in the center of the bottom of the mold with 502 glue. Add 5 / 1000 volume accelerator to 1 volume unsaturated polyurethane resin, and then add 9 / 1000 volume The curing agent, after stirring evenly, cool it down to 25°C with ice water and pour it into the mold, and take it out after solidification.
Embodiment 3
[0023] Select a rose with a stem of about 10cm, bury it in silica gel powder (Shanghai test, 200-300 mesh), take it out after 24 hours, carefully remove the silica gel powder on the surface of the rose with a small brush, and insert a An iron wire of suitable size is used to increase the strength of the flower stem. Fix the rose in the center of the bottom of the mold with 502 glue. Add 5 / 1000 volume accelerator to 1 volume unsaturated polyurethane resin, and then add 9 / 1000 volume The curing agent, after stirring evenly, cool down to 28°C and pour it into the mold, and take it out after solidification.