Repairing agent for damaged skin and preparation method thereof
A repairing agent and skin technology, applied in the field of skin repairing agent and its preparation, can solve the problems of excessive heavy metals, damage, hormone abuse, etc., and achieve the effect of preventing moisture distribution, beautiful luster, and promoting tissue growth
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0104] A repair agent for damaged skin, composed of the following ingredients by mass percentage:
[0105] β-glucan 5;
[0106] Propylene glycol 10;
[0107] Golden Chamomile Extract 5;
[0108] Portulaca extract 5;
[0109] Aloe extract 5;
[0110] Chitosan 5;
[0111] Panthenol 3;
[0112] Sodium Hyaluronate 0.3;
[0113] Oligopeptide-1 0.2;
[0114] Allantoin 0.2;
[0115] Water balance.
[0116] The specific method steps are as follows:
[0117] a. Take an appropriate amount of purified water and heat it to 100°C for 60 minutes;
[0118] b. Cool the high-temperature hot water obtained in step a to 70°C, add the formula amount of propylene glycol and sodium hyaluronate to the hot water at 70°C, stir evenly to make it completely dissolved;
[0119] c. Continue to cool the water at 70°C obtained in step b to 55°C, add the formulated amount of allantoin, and stir to dissolve completely.
[0120] d. Continue to cool the 55°C water obtained in step c to 45°C, and add the formula amount of golden cha...
Embodiment 2
[0125] A repair agent for damaged skin, composed of the following ingredients by mass percentage:
[0126] β-glucan 6;
[0127] Propylene glycol 15;
[0128] Golden Chamomile Extract 7;
[0129] Purslane extract 7;
[0130] Aloe extract 7;
[0131] Chitosan 4;
[0132] Panthenol 4;
[0133] Sodium Hyaluronate 0.3;
[0134] Oligopeptide-1 0.2;
[0135] Allantoin 0.2;
[0136] Water balance.
[0137] The specific method steps are as follows:
[0138] a. Take an appropriate amount of purified water and heat it to 100°C for 50 minutes;
[0139] b. The high-temperature hot water obtained in step a is cooled to 65°C, and the formula amount of propylene glycol and sodium hyaluronate are added to the 65°C hot water, and the mixture is stirred evenly to melt completely;
[0140] c. Continue to cool the 65°C water obtained in step b to 50°C, add the formulated amount of allantoin, and stir to dissolve completely.
[0141] d. Continue to cool the 50°C water obtained in step c to 45°C, and add the formula amo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com