A filter material and filter technology, applied in the field of filter material preparation, can solve the problems of serious stone powder, air pollution, endangering human health, etc., and achieve the effect of high purification efficiency retention, good corrosion resistance effect and prolonging service life.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] A filter filter material capable of removing fine dust in the air, comprising the following steps:
[0015] (1) Preparation of raw materials, by weight, including 25 parts of block copolymerized polypropylene, 15 parts of 2-hydroxypropyl methacrylate, 3 parts of antioxidant, 7 parts of inorganic fiber, 1.5 parts of fatty acid, and 8 parts of magnesium hydroxide 5 parts, 5 parts of talcum powder, 2 parts of glycerol triglyceride, 3 parts of nitrated chitosan, 8 parts of processing material of black wattle bark powder;
[0016] Wherein, the black wattle bark powder processing material is to crush the black wattle bark, add polyether propylene oxide equivalent to 1.65 times its weight, and stir for 35 minutes at a temperature of 30°C. , ball milled for 1.5 hours under a nitrogen atmosphere at a temperature of 90°C to obtain a powder with a particle size of 90 mesh;
[0017] (2) After the above raw materials are mixed, the mud is smelted under vacuum conditions at a temper...
Embodiment 2
[0021] A filter filter material capable of removing fine dust in the air, comprising the following steps:
[0022] (1) Preparation of raw materials, by weight, including 22 parts of block copolymerized polypropylene, 18 parts of 2-hydroxypropyl methacrylate, 2 parts of antioxidant, 8 parts of inorganic fiber, 1 part of fatty acid, and 10 parts of magnesium hydroxide 1 part, 6 parts of talcum powder, 1 part of glycerol triglyceride, 2 parts of nitrated chitosan, 10 parts of black wattle bark powder processing material;
[0023] Wherein, the black wattle bark powder processing material is to crush the black wattle bark, add polyether propylene oxide equivalent to 1.8 times its weight, and stir for 40 minutes at a temperature of 35°C. , ball milled for 2 hours under a nitrogen atmosphere at a temperature of 100°C to obtain a powder with a particle size of 80 mesh;
[0024] (2) After the above raw materials are mixed, the mud is smelted under vacuum conditions at a temperature of...
Embodiment 3
[0028] A filter filter material capable of removing fine dust in the air, comprising the following steps:
[0029] (1) Preparation of raw materials, by weight, including 28 parts of block copolymerized polypropylene, 12 parts of 2-hydroxypropyl methacrylate, 4 parts of antioxidant, 6 parts of inorganic fiber, 2 parts of fatty acid, and 6 parts of magnesium hydroxide 4 parts, 4 parts of talcum powder, 3 parts of glycerol triglyceride, 4 parts of nitrated chitosan, 6 parts of processing material of black wattle bark powder;
[0030] Wherein, the black wattle bark powder processing material is to crush the black wattle bark, add polyether propylene oxide equivalent to 1.5 times its weight, and stir for 30 minutes at a temperature of 25°C. , ball milled for 1 hour under a nitrogen atmosphere at a temperature of 80°C to obtain a powder with a particle size of 100 mesh;
[0031] (2) After the above raw materials are mixed, the mud is smelted under vacuum conditions at a temperature...