Preparation method of drug-loaded wound dressing
A wound dressing and drug-loading technology, applied in medical science, bandages, absorbent pads, etc., can solve the problems of secondary injury, wound exudate cannot be absorbed, and slow down the scab rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Weigh 18 kg of non-ionic polyurethane hydrogel particles, 25 kg of thermoplastic polyurethane particles with a Shore hardness of 50A, and 120 kg of N,N-dimethylformamide in a reactor, heat to 50°C and stir Completely dissolve the polyurethane hydrogel particles and thermoplastic polyurethane particles, and obtain a polyurethane solution after cooling; add 40 kg of 500-mesh Yunnan Baiyao powder, and stir evenly with a high-speed mixer to obtain a solid-liquid mixture; carry out 0.5h decompression and defoaming treatment Then quickly apply the solid-liquid mixture on the release paper, then immerse the release paper in deionized water, put it in a drying oven after solidification and form a film, and dry it at 50°C for 1 hour, and remove the release paper after cooling, that is The solid-loaded Yunnan Baiyao film was obtained; the solid-loaded Yunnan Baiyao film was immersed in the extract of Zizhucao (the content of Zizhucao extract was 5.0%) for 3 hours, and then vacuum ...
Embodiment 2
[0024] Weigh 10 kg of non-ionic polyurethane hydrogel particles, 42 kg of thermoplastic polyurethane particles with a Shore hardness of 50A, and 120 kg of N,N-dimethylformamide in a reactor, heat to 60°C and stir Completely dissolve the polyurethane hydrogel particles and thermoplastic polyurethane particles, and obtain a polyurethane solution after cooling; add 40 kg of 1000-mesh Yunnan Baiyao powder, and stir evenly with a high-speed stirrer to obtain a solid-liquid mixture; carry out 0.5h decompression and defoaming treatment Then quickly apply the solid-liquid mixture on the release paper, then immerse the release paper in deionized water, place it in a drying oven after solidification and form a film, and dry it at 50°C for 2 hours, and remove the release paper after cooling, that is The solid-loaded Yunnan Baiyao film was obtained; the solid-loaded Yunnan Baiyao film was immersed in the extract of Zizhucao (the content of Zizhucao extract was 10.0%) for 3 hours, and then ...
Embodiment 3
[0027] Weigh 10 kg of non-ionic polyurethane hydrogel particles, 25 kg of thermoplastic polyurethane particles with a Shore hardness of 60A, and 120 kg of N,N-dimethylacetamide in a reactor, heat to 70°C and stir Completely dissolve the polyurethane hydrogel particles and thermoplastic polyurethane particles, and obtain a polyurethane solution after cooling; add 40 kg of 1500-mesh Yunnan Baiyao powder, and stir evenly with a high-speed mixer to obtain a solid-liquid mixture; carry out 0.5h decompression and defoaming treatment Afterwards, quickly apply the solid-liquid mixture on the release paper, then immerse the release paper in deionized water, place it in a drying oven after solidification and form a film, and dry it at 50°C for 1 hour, and remove the release paper after cooling to obtain Solid-loaded Yunnan Baiyao film; soak the solid-loaded Yunnan Baiyao film in the extract of Zizhucao (the content of Zizhucao extract is 6.0%) for 3 hours, and then vacuum freeze-dry to o...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Shore hardness | aaaaa | aaaaa |
Shore hardness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com