Arctiin compound entrapped local skin external preparation based on solid particle emulsification technology and preparation method and application of arctiin compound entrapped local skin external preparation
An external preparation, the technology of arctiside, applied in the field of preparation, can solve the problems of complex process, skin safety problem, weak effect of stabilizing emulsion system, etc.
Patent Information
- Authority / Receiving Office
- CN · China
- Current Assignee / Owner
- Publication Date
- 2021-05-21
Smart Images

Figure 1 
Figure 2 
Figure 3
Abstract
Description
technical field
[0001] The invention relates to the field of preparations, in particular to a topical skin external preparation loaded with arctiin compounds based on solid particle emulsification technology and its preparation method and application. Background technique
[0002] Emulsions are one of the main dosage forms for topical therapy, with the advantage of protecting the encapsulated drug while increasing its solubility and improving drug skin penetration behavior. Since the emulsion is a thermodynamically unstable system, it is necessary to use a stabilizer to form a stable system and ensure its long-term stability. To date, most emulsions have relied on synthetic surfactants for stabilization. More and more studies have shown that the application of surfactants will lead to skin safety problems, while their role in stabilizing the emulsion system is not strong and the cost is high.
[0003] In addition, the traditional emulsion process is relatively complicated,...
Examples
Embodiment 1
[0083] 1. an external preparation matrix of arctiin compounds, comprising:
[0084] 244FP 1.5g, diethylene glycol monoethyl ether 11.5g, hydroxypropyl cellulose 2g, light liquid paraffin 25g, water 60g.
[0085] The preparation method of above-mentioned external preparation matrix comprises the following steps:
[0086] Add water and hydroxypropyl cellulose to diethylene glycol monoethyl ether to fully swell to obtain an aqueous phase; Disperse 244FP in light liquid paraffin to obtain an oil phase; add the oil phase to the water phase and homogenize at a speed of 15,000 rpm for 5 minutes to obtain the product.
[0087] 2. An external preparation of arctiin compounds, comprising:
[0088] Arctigenin 5g, 244FP 1.5g, diethylene glycol monoethyl ether 11.5g, hydroxypropyl cellulose 2g, light liquid paraffin 25g, water 60g.
[0089] The preparation method of above-mentioned external preparation comprises the steps:
[0090] Dissolving arctigenin in the prescription amount ...
Embodiment 2
[0092] An external preparation of arctiin compounds, comprising:
[0093] Arctiin 5g, 244FP 1.5g, diethylene glycol monoethyl ether 11.5g, hydroxypropyl cellulose 2g, light liquid paraffin 25g, water 60g.
[0094] The preparation method of above-mentioned external preparation comprises the steps:
[0095] Disperse the arctiin of the prescribed amount in diethylene glycol monoethyl ether, add water and hydroxypropyl cellulose, fully swell, and obtain the water phase; Disperse 244FP in light liquid paraffin to obtain an oil phase; add the oil phase to the water phase and homogenize at a speed of 15,000 rpm for 5 minutes to obtain the product.
Embodiment 3
[0097] An external preparation of arctiin compounds, comprising:
[0098] Arctigenin 2.5g, MCG 591P 5g, propylene glycol 20g, povidone K30 5g, simethicone 10g, water 57.5g.
[0099] The preparation method of above-mentioned external preparation comprises the steps:
[0100] Dissolve the prescribed amount of arctigenin in propylene glycol, add water and povidone K30, fully dissolve, and then add MCG 591P is uniformly dispersed to obtain a water phase; add simethicone as an oil phase to the water phase, and homogenize at a speed of 7000rpm for 20 minutes to obtain the product.