Embodiment 1
[0023] A cyanobacteria scavenging agent with pumice as a carrier, which is prepared from cerium nitrate solution, sodium hydroxide solution and massive pumice raw materials, the addition of sodium hydroxide solution is 1% of the volume of the cerium nitrate solution, and the volume of the massive pumice The addition amount is 5% of the total mass of the cerium nitrate solution and the sodium hydroxide solution; wherein, the mass concentration of the cerium nitrate solution is 0.2%, and the mass concentration of the sodium hydroxide solution is 5%; the block pumice is: the pumice is broken into a block with a diameter of 0.5 cm, stirred and washed with 8% sodium hydroxide solution for 1.5 h, then washed until neutral, and dried to obtain block pumice.
[0024] Above-mentioned a kind of preparation method taking pumice as the cyanobacteria scavenging agent of carrier, it comprises the steps:
[0025] 1) Breaking the pumice into blocks with a diameter of 0.5 cm, stirring and wash...
Embodiment 2
[0030]A cyanobacteria scavenging agent with pumice as a carrier, which is prepared from cerium nitrate solution, sodium hydroxide solution and massive pumice raw materials, the addition of sodium hydroxide solution is 5% of the volume of the cerium nitrate solution, and the volume of the massive pumice The addition amount is 10% of the total mass of the cerium nitrate solution and the sodium hydroxide solution; wherein, the mass concentration of the cerium nitrate solution is 0.5%, and the mass concentration of the sodium hydroxide solution is 10%; the block pumice is: the pumice is broken into blocks with a diameter of 3 cm, stirred and washed with 12% sodium hydroxide solution for 2.5 hours, then washed until neutral, and dried to obtain block pumice.
[0031] Above-mentioned a kind of preparation method taking pumice as the cyanobacteria scavenging agent of carrier, it comprises the steps:
[0032] 1) Breaking the pumice into blocks with a diameter of 3 cm, stirring and was...
Embodiment 3
[0037] A cyanobacteria scavenging agent with pumice as a carrier, which is prepared from cerium nitrate solution, sodium hydroxide solution and massive pumice raw materials, the addition of sodium hydroxide solution is 3% of the volume of the cerium nitrate solution, and the volume of the massive pumice The addition amount is 8% of the total mass of the cerium nitrate solution and the sodium hydroxide solution; wherein, the mass concentration of the cerium nitrate solution is 0.4%, and the mass concentration of the sodium hydroxide solution is 8%; the block pumice is: the pumice is broken into a block with a diameter of 1 cm, stirred and washed with 10% sodium hydroxide solution for 2.0 h, then washed until neutral, and dried to obtain block pumice.
[0038] Above-mentioned a kind of preparation method taking pumice as the cyanobacteria scavenging agent of carrier, it comprises the steps:
[0039] 1) Breaking the pumice into blocks with a diameter of 1 cm, stirring and washing...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com