Acid-washing corrosion-inhibition fog inhibitor
A fog inhibitor and corrosion inhibitor technology, applied in the field of fog inhibitor, can solve the problems of unstable foam layer formation, unsuitable for industrialized generation, large addition amount, etc. good effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0035] The preparation method of fog suppressant, the steps are as follows:
[0036] 1. First dissolve the solid material and water;
[0037] Solid material: hexamethylenetetramine, sodium gluconate, oxalic acid, sodium lauryl sulfate, sodium dodecylbenzenesulfonate, sodium benzoate
[0038] 2. Then add the liquid material and stir;
[0039] Liquid material: fatty alcohol polyoxyethylene ether sulfate, octadecethoxyethylene ether, alkylphenol polyoxyethylene ether, penetrating agent
[0040] 3. Add additives and mix thoroughly;
[0041] Additives include: coconut oil fatty acid diethanolamide, foam stabilizer, essence, fatty alcohol polyoxyethylene ether, leveling agent
[0042] 4. After mixing evenly, let it stand for 4-8 hours;
[0043] 5. Discharge.
Embodiment 1
[0045] A pickling anti-corrosion anti-fog agent, comprising the following components and weight percentages:
[0046]
[0047]
[0048] The preparation method of fog suppressant, the steps are as follows:
[0049] 1. First dissolve the solid material and water;
[0050] Solid material: hexamethylenetetramine, sodium gluconate, oxalic acid, sodium lauryl sulfate, sodium dodecylbenzenesulfonate, sodium benzoate;
[0051] 2. Then add the liquid material and stir;
[0052] Liquid material: fatty alcohol polyoxyethylene ether sulfate, octadecyl polyoxyethylene ether, alkylphenol polyoxyethylene ether, penetrating agent;
[0053] 3. Add additives and mix thoroughly;
[0054] Additives include: coconut oil fatty acid diethanolamide, foam stabilizer, essence, fatty alcohol polyoxyethylene ether, leveling agent;
[0055] 4. After mixing evenly, let it stand for 4-8 hours;
[0056] 5. Discharge.
Embodiment 2
[0058] A pickling anti-corrosion anti-fog agent, comprising the following components and weight percentages:
[0059]
[0060]
[0061] The preparation method is the same as in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com