Production process method for wooden door
A production process and wooden door technology, applied in wood processing equipment, manufacturing tools, etc., can solve the problems of cumbersome production process and inability to improve production efficiency, and achieve the effect of simplifying steps and improving production efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] Embodiment 1: Step 1: blanking. When rough cutting, increase the length and width by 10mm.
[0026] Step 2: Group Box. The four corners are square, and the length and width are increased by 10mm. The middle is filled with Sauerland hollow particleboard, and lock wood is added.
[0027] Step 3: Heat Press. Before each workpiece that needs to be hot-pressed, clean the hot-pressing plate and the workpiece, confirm that there are no impurities, set the hot-pressing temperature and pressure, and slowly put the workpiece in; the placed workpieces are arranged in an orderly manner, and each part is stressed Uniform; each hot pressing should fill all positions as much as possible, and ensure that the thickness of each layer of boards is the same as the cladding material of each layer, and the cladding material cannot be repeated; in order to prevent the glue from drying, each loading should be completed within two minutes, and it must be correct And when it is safe, start th...
Embodiment 2
[0035] Example 2: If the material is combined, indicate the material of the veneer and indicate the type of door combination.
Embodiment 3
[0036] Embodiment 3: The width specification of the outer frame is 800-2000mm, and the surface board is 6mm medium density board; the lock box replaces the lock wood.