Clothing compression bag and preparation method thereof
A technology for compressing bags and making methods, applied in chemical instruments and methods, bags, sacks, etc., can solve the problems of being susceptible to moisture and occupying space for idle clothes, and achieve the effects of large storage space, long service life and convenient cleaning.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A clothing compression bag is composed of PA layer, adhesive layer and PE layer sequentially from outside to inside. Wherein, the adhesive layer is made of a composite adhesive, and the mass ratio of the composite adhesive is 766 glue (purchased from Jiangsu Jinhu County Bairuite Chemical Co., Ltd.): polyurethane curing agent: B Ester = 10:2:13. The thickness of the PA layer is 21um; the thickness of the PE layer is 35um.
[0019] The method for making the above-mentioned clothing compression bag, the specific steps are as follows:
[0020] a. Dry the PA layer and PE layer with a composite adhesive, and then pass through a drying tunnel with a length of 3 to 4m at a speed of 80m / min. ℃, 60℃, 70℃, after drying, the composite adhesive is an adhesive layer, and the mass ratio of the composite adhesive is 766 glue (purchased from Jiangsu Jinhu County Bairuite Chemical Co., Ltd.): polyurethane Curing agent: ethyl ester=10:2:13;
[0021] b. After cutting the material obt...
Embodiment 2
[0024] A clothing compression bag is composed of PA layer, adhesive layer and PE layer sequentially from outside to inside. Wherein, the adhesive layer is made of a composite adhesive, and the mass ratio of the composite adhesive is 766 glue (purchased from Jiangsu Jinhu County Bairuite Chemical Co., Ltd.): polyurethane curing agent: B Ester = 8:1:11. The thickness of the PA layer is 12um; the thickness of the PE layer is 20um.
[0025] The method for making the above-mentioned clothing compression bag, the specific steps are as follows:
[0026] a. Dry the PA layer and PE layer with a composite adhesive, and then pass through a drying tunnel with a length of 3 to 4m at a speed of 80m / min. ℃, 60℃, 70℃, the composite adhesive is an adhesive layer after drying, and the mass ratio of the composite adhesive is 766 glue (purchased from Jiangsu Jinhu County Bairuite Chemical Co., Ltd.) : polyurethane curing agent: ethyl ester = 8: 1: 11;
[0027] b. After cutting the material ob...
Embodiment 3
[0030] A clothing compression bag is composed of PA layer, adhesive layer and PE layer sequentially from outside to inside. Wherein, the adhesive layer is made of a composite adhesive, and the mass ratio of the composite adhesive is 766 glue (purchased from Jiangsu Jinhu County Bairuite Chemical Co., Ltd.): polyurethane curing agent: B Ester = 12:3:15. The thickness of the PA layer is 30um; the thickness of the PE layer is 50um.
[0031] The method for making the above-mentioned clothing compression bag, the specific steps are as follows:
[0032] a. Dry the PA layer and PE layer with a composite adhesive, and then pass through a drying tunnel with a length of 3 to 4m at a speed of 80m / min. ℃, 60℃, 70℃, the composite adhesive is an adhesive layer after drying, and the mass ratio of the composite adhesive is 766 glue (purchased from Jiangsu Jinhu County Bairuite Chemical Co., Ltd.) : polyurethane curing agent: ethyl ester = 12: 3: 15;
[0033] b. After cutting the material...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More