[0013] The raw materials are passed through a 200-mesh sieve, and 30 parts of bamboo charcoal powder, 20 parts of potassium perchlorate, 15 parts of nano-silver powder, 10 parts of nano-rare earth oxide, 4 parts of carbon powder, 4 parts of titanium sponge powder and 3 parts of agarwood powder are taken by weight. After spraying water accounting for 8% of the total weight of the medicament, mix evenly, charge and insert to make firecrackers.
Embodiment 2
[0015] Pass the raw materials through a 200-mesh sieve, and take 30 parts by weight of bamboo charcoal powder, 10 parts of potassium perchlorate, 10 parts of nano-silver powder, 15 parts of nano-rare earth oxide, 2 parts of carbon powder, 2 parts of titanium sponge powder, and 4 parts of agarwood powder. After spraying water accounting for 8% of the total weight of the medicament, mix evenly, charge and insert to make firecrackers.
Embodiment 3
[0017] The raw materials are passed through a 200-mesh sieve, and 30 parts of bamboo charcoal powder, 30 parts of potassium perchlorate, 20 parts of nano-silver powder, 5 parts of nano-rare earth oxide, 6 parts of carbon powder, 5 parts of titanium sponge powder and 1 part of agarwood powder are taken by weight. After spraying water accounting for 8% of the total weight of the medicament, mix evenly, charge and insert to make firecrackers.
[0018] Detected by the National Fireworks and Firecrackers Product Quality Supervision and Inspection Center, the light smoke and sulfur-free firecrackers prepared by the above-mentioned embodiments have a friction sensitivity of 0, an impact sensitivity of 0, and a moisture absorption rate≤1.12% (the friction sensitivity test method is in accordance with SN0545-1996). 5.5; impact sensitivity test method according to 5.4 in SN0545-1996; hygroscopicity according to QB / T1914.5 method). According to the standard of GB10631-2004 "Safety and Qu...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
water absorption | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com