Whitening glaze slurry for high-strength ceramics and preparation method thereof

A whitening glaze, high-strength technology, applied in the field of ceramic materials, can solve the problems of poor mechanical strength and flatness, poor whitening effect, low service life, etc., to achieve increased strength, improved brightness and gloss, and improved service life. Effect

Active Publication Date: 2018-12-04
JIAXIAN HONGDA PORCELAIN CO LTD
View PDF4 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] In order to solve the problems of poor whitening effect, high cost of whitening, low covering ability, poor mechanical strength and smoothness of the glazed surface of ceramic products after spraying with glaze slurry, and low service life in the existing glaze slurry for ceramics, the present invention The purpose of the present invention is to provide a whitening glaze slurry for high-strength ceramics and a preparation method thereof. After spraying the glaze slurry on a ceramic body and making a ceramic product, the whiteness, brightness and gloss of the ceramic product can be improved, and It can enhance the mechanical strength and flatness of the glazed surface of ceramic products, and improve the service life of ceramic products

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0023] A whitening glaze slurry for high-strength ceramics is formed by mixing raw materials and water through ball milling. According to the weight ratio, the raw materials are composed of 16 parts of potassium feldspar, 15 parts of calcite, 16 parts of quartz, 10 parts of frit, 1 part of Soda ash, 10 parts of calcium carbonate, 0.5 part of dolomite, 4 parts of whitening agent and 0.5 part of strengthening agent are mainly composed of 50 parts of kaolin, 50 parts of titanium dioxide, 1 part of hardening agent according to the weight ratio. Calcium fatty acid and 2 parts of y-chloropropyl trimethoxysilane, and the reinforcing agent is made of 10 parts of hydroxyapatite, 10 parts of calcined talc and 0.2 parts of aluminum-zirconium coupling agent according to the weight ratio.

[0024] In the preparation method of a whitening glaze slurry for high-strength ceramics, each material is weighed and selected according to the above ratio, and then the whitening agent and the strengthe...

Embodiment 2

[0035] A whitening glaze slurry for high-strength ceramics is formed by mixing raw materials and water through ball milling. According to the weight ratio, the raw materials are composed of 19 parts of potassium feldspar, 17 parts of calcite, 18 parts of quartz, 12 parts of frit, 3 parts Soda ash, 12 parts of calcium carbonate, 1.5 parts of dolomite, 5 parts of whitening agent and 1.5 parts of strengthening agent are mainly composed of 60 parts of kaolin, 60 parts of titanium dioxide, 1.5 parts of hardening agent according to the weight ratio. Calcium fatty acid and 3 parts of y-chloropropyl trimethoxysilane, and the reinforcing agent is made of 12 parts of hydroxyapatite, 12 parts of calcined talc and 0.3 parts of aluminum-zirconium coupling agent according to the weight ratio.

[0036] In the preparation method of a whitening glaze slurry for high-strength ceramics, each material is weighed and selected according to the above ratio, and then the whitening agent and the streng...

Embodiment 3

[0047] A whitening glaze slurry for high-strength ceramics is formed by mixing raw materials and water through ball milling. According to the weight ratio, the raw materials are composed of 22 parts of potassium feldspar, 19 parts of calcite, 20 parts of quartz, 14 parts of frit, 5 parts of Soda ash, 14 parts of calcium carbonate, 2.5 parts of dolomite, 6 parts of whitening agent and 2.5 parts of strengthening agent are mainly composed of 70 parts of kaolin, 70 parts of titanium dioxide, 2 parts of hardening agent according to the weight ratio. Calcium fatty acid and 4 parts of y-chloropropyl trimethoxysilane, and the strengthening agent is made of 14 parts of hydroxyapatite, 20 parts of calcined talc and 0.4 parts of aluminum-zirconium coupling agent according to the weight ratio.

[0048] In the preparation method of a whitening glaze slurry for high-strength ceramics, each material is weighed and selected according to the above ratio, and then the whitening agent and the str...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses high-strength whitening glaze slurry for ceramic and a preparation method of the high-strength whitening glaze slurry. The glaze slurry is prepared from raw materials and water through mixing and ball milling; the raw materials comprise, in parts by weight, 16-22 parts of potash feldspar, 15-19 parts of calcite, 16-20 parts of quartz, 10-14 parts of frit, 1-5 parts of sodium carbonate, 10-14 parts of calcium carbonate, 0.5-2.5 parts of dolomite, 4-6 parts of a whitening agent and 0.5-2.5 parts of a reinforcing agent, wherein the whitening agent is prepared from 50-70 parts of kaoline, 50-70 parts of titanium dioxide, 1-2 parts of calcium stearate and 2-4 parts of gamma-chloropropyltrimethoxysilane; the reinforcing agent is prepared from, in parts by weight, 10-14 parts of hydroxyapatite, 10-20 parts of calcined talc and 0.2-0.4 parts of an aluminum zirconium coupling agent. The high-strength whitening glaze slurry for the ceramic adopts reasonable materials, a preparation method is simple, the production cost is low, the performance is good, and the high-strength whitening glaze slurry is worth popularization and application.

Description

technical field [0001] The invention relates to the technical field of ceramic materials, in particular to a whitening glaze slurry for high-strength ceramics and a preparation method thereof. Background technique [0002] Glaze is a glossy glass-like thin layer covering the surface of the ceramic body, and its function is to improve the physical and chemical properties of the body surface. Generally, the surface of the ceramic body is loose and porous, rough and dull, moisture absorption and easy to be stained and other shortcomings affect the mechanical properties of the product, and spraying glaze slurry on the ceramic body can overcome these shortcomings and improve the mechanical properties of the product and increase the strength of the product. , hardness and thermal stability. Based on the role of glaze slurry on ceramic products, the importance of glaze slurry in the ceramic industry is constantly being highlighted and enhanced, and the material and preparation met...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C03C8/20C04B41/86
CPCC03C8/20C04B41/5022C04B41/86C04B35/00
Inventor 李浩伟
Owner JIAXIAN HONGDA PORCELAIN CO LTD
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products