Curtain wall steel structure mounting method
An installation method and technology of steel structure, applied in the direction of walls, building components, building structures, etc., can solve the problems of reduced service life, no anti-oxidation treatment, and reduced anti-rust effect of zinc layer.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0037] The curtain wall steel structure installation method includes the following steps,
[0038] S1. Manually or mechanically derust the outer surface of the steel. Every time a part of the derusting is completed, the derusted part is coated with carbon powder, and the thickness of the carbon powder is 20 microns;
[0039] S2. Use hoisting equipment to hoist the steel directly above the hot-melt zinc pool; the distance between the steel and the upper surface of the hot-melt zinc pool is to ensure that the outer surface temperature of the steel is 300 degrees Celsius; use an ignition device to align the outer surface of the steel so that the carbon powder starts to burn ; After the carbon powder on the outer surface of the steel is completely burnt, the steel is hot-dipped in the zinc pool for galvanizing using hoisting equipment; the thickness of the zinc layer on the outer surface of the steel is 110 microns;
[0040] S3. Divide positioning points on the outer surface of th...
Embodiment 2
[0052] The curtain wall steel structure installation method includes the following steps,
[0053] S1. Manually or mechanically derust the outer surface of the steel. Every time a part of the derusting is completed, the derusted part is coated with carbon powder, and the thickness of the carbon powder is 20 microns;
[0054] S2. Use hoisting equipment to hoist the steel directly above the hot-melt zinc pool; the distance between the steel and the upper surface of the hot-melt zinc pool is to ensure that the outer surface temperature of the steel is 400 degrees Celsius; use an ignition device to align the outer surface of the steel so that the carbon powder starts to burn ; After the carbon powder on the outer surface of the steel is completely burnt, the steel is hot-dipped in the zinc pool for galvanizing using hoisting equipment; the thickness of the zinc layer on the outer surface of the steel is 110 microns;
[0055] S3. Divide positioning points on the outer surface of th...
Embodiment 3
[0067] The curtain wall steel structure installation method includes the following steps,
[0068] S1. Manually or mechanically derust the outer surface of the steel. Every time a part of the derusting is completed, the derusted part is coated with carbon powder, and the thickness of the carbon powder is 20 microns;
[0069] S2. Use hoisting equipment to hoist the steel directly above the hot-melt zinc pool; the distance between the steel and the upper surface of the hot-melt zinc pool is to ensure that the outer surface temperature of the steel is 350 degrees Celsius; use an ignition device to align the outer surface of the steel so that the carbon powder starts to burn ; After the carbon powder on the outer surface of the steel is completely burnt, the steel is hot-dipped in the zinc pool for galvanizing using hoisting equipment; the thickness of the zinc layer on the outer surface of the steel is 110 microns;
[0070] S3. Divide positioning points on the outer surface of th...
PUM
Property | Measurement | Unit |
---|---|---|
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com