A technology for lithium-ion batteries and positive electrode materials, which is applied in battery electrodes, secondary batteries, circuits, etc., can solve the problems affecting the electrochemical performance of lithium-ion batteries, large gaps, and large contact resistance, and achieve excellent electrochemical performance. The effect of dispersing difficulty and smooth filling
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0038] Embodiment 1, differs from comparative example in that this embodiment comprises the following steps:
[0039] Step 1, dry-mix lithium metal powder, lithium iron phosphate with a diameter of 100 nm, and graphite particles with a particle size of 6 μm until uniform;
[0040] Step 2, select the electrolyte solution with lithium hexafluorophosphate as the salt and PC as the solvent, add it to the above mixture and continue stirring. At this time, under the action of metal lithium powder, PC will peel off the graphite particles to form an open structure, and at the same time, the primary particles of the positive electrode will fill into the mouth structure;
[0041] Step 3, after the filling is completed, the electrolyte components are removed, coated and carbonized to obtain the positive electrode material of the lithium-ion battery.
[0042] The rest are the same as the comparative example and will not be repeated here.
Embodiment 2
[0043] Embodiment 2 is different from the comparative example in that the present embodiment comprises the following steps:
[0044] Step 1, mixing and kneading lithium iron phosphate with a diameter of 100 nm, graphite particles with a particle size of 6 μm, and lithium hexafluorophosphate as the salt and PC as the solvent until uniform;
[0045] Step 2, assemble the counter electrode with lithium iron phosphate as the power source material, and then form the counter electrode with the material obtained in step 1, connect the external circuit, charge with a current of 1A, peel off the graphite particles, and form a graphite sheet opening structure; Afterwards, the nano-positive primary particles will continue to fill into the opening structure of the graphite sheet;
[0046] Step 3, after the filling is completed, the electrolyte components are removed, coated and carbonized to obtain the positive electrode material of the lithium-ion battery.
[0047] The rest are the same ...
Embodiment 3
[0048] Embodiment 3 is different from Embodiment 1 in that this embodiment includes the following steps:
[0049] Step 1, dry mixing and kneading lithium metal powder, lithium iron phosphate with a diameter of 100 nm, methyl methacrylate, sodium lauryl sulfate, and graphite particles with a particle size of 6 μm until uniform;
[0050] Step 2, select the electrolyte solution with lithium hexafluorophosphate as the salt and PC as the solvent, add it to the above mixture and continue stirring. At this time, under the action of metal lithium powder, PC will peel off the graphite particles to form an open structure, and at the same time, the primary particles of the positive electrode will fill into the opening structure;
[0051] Step 3, dissolving tert-butyl peroxybenzoate in PC to form an initiator solution, after the filling described in step 3 is completed, add the initiator solution, increase the temperature, and promote the polymerization reaction of the polymer monomer, on...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com