A diversion plate and combined technology, applied in welding equipment, manufacturing tools, overhead lines/cable equipment, etc., can solve the problems of difficult disassembly of the diversion plate, heating of the diversion plate clamp, poor contact of the diversion plate, etc., to solve the problem of difficult disassembly, The effect of easy disassembly and replacement
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0041] The present application provides an embodiment. This embodiment provides a method for disassembling the drain plate, which includes the following steps: performing low-temperature treatment on the two drain plates 1 welded together by tin solder, and then treating the two drain plates 1 with alcohol. Rinse the connection of the board 1 to dissolve the residual flux, and finally disassemble and separate the two drain boards 1 welded together by tin solder. Soak in cooling liquid stabilized at 13°C, so that the solder layer 3 between the two drain plates 1 gradually turns into a broken powder, and the time required for the entire process of dismantling the drain plate 1 is 24 hours;
[0042] Wherein, the tin solder includes tin powder with a mass percentage of 99.3% and copper powder with a mass percentage of 0.7%.
Embodiment 2
[0044] The present application provides another embodiment. This embodiment provides another method for disassembling the drain plate, which includes the following steps: performing low-temperature treatment on the two drain plates 1 welded together by tin solder, and then treating the two drain plates 1 with alcohol. Rinse the joints of the two drain plates 1 to dissolve the residual flux, and finally disassemble and separate the two drain plates 1 welded together by tin solder. Material wrapping dry ice covers the two drain plates 1, so that the solder layer 3 between the two drain plates 1 gradually changes into a broken powder, and the time required for the entire process of dismantling the drain plate 1 is 1h; The solder includes tin powder with a mass percentage of 98.3% and copper powder with a mass percentage of 1.7%.