A preparation process and glass technology, which is applied in the field of preparation process of concave silk screen glass, can solve the problems of screen screen making, unsatisfactory selection of mesh number, and restrictions on the production of concave silk screen glass printing, etc., and achieve obvious concave and convex effects , a wide range of effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A preparation process for concave screen printing glass, the process comprises the following steps:
[0024] (1) Coating the 8500 series ink a purchased from France Dolby Ink Company on the screen whose mesh number is 100 mesh and whose mesh is polyester mesh, makes the thickness of ink a 20 μm, and then prints on the glass surface, dry thoroughly at 100°C for 36 hours,
[0025] (2) On the surface of the glass obtained in step (1), print the ink b of Jinhaoli Ink Co., Ltd. with pearlescent or silver paste series with strong fineness and scintillation, and dry it thoroughly at 100° C. for 36 hours;
[0026] (3) Spray paint on the surface of the glass obtained in step (2), and dry to obtain the product.
Embodiment 2
[0028] A preparation process for concave screen printing glass, the process comprises the following steps:
[0029] (1) Coat the 1500 series ink a purchased from French Dolby Ink Company on the screen whose screen mesh number is 250 mesh, and the mesh is polyester mesh, so that the thickness of the ink a is 500 μm, and then printed on the glass On the surface, dry thoroughly at 200°C for 10 hours,
[0030] (2) On the surface of the glass obtained in step (1), print the EAP series ink b purchased from the French Dolby Ink Company with pearlescent or silver paste series with strong fineness and sparkle, and dry thoroughly at 200°C for 10 hours ;
[0031] (3) Spray paint on the surface of the glass obtained in step (2), and dry to obtain the product.
Embodiment 3
[0033] A preparation process for concave screen printing glass, the process comprises the following steps:
[0034] (1) Coat the 8500 / 100 series ink a purchased from French Dolby Ink Company on the screen whose mesh number is 150 mesh, and the mesh yarn is polyester mesh, so that the thickness of the ink a is 100 μm, and then print On the glass surface, dry thoroughly at 120°C for 24 hours,
[0035] (2) 8500 / 100 series ink b purchased from French Dolby Ink Company with pearl luster or silver paste series with strong fineness and scintillation on the surface of the glass obtained in step (1), dried at 120°C for 24 hours dry thoroughly;
[0036] (3) Spray paint on the surface of the glass obtained in step (2), and dry to obtain the product.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com