Tripoli composition
A technology of diatomite and composition, applied in the field of diatomite composition, can solve the problems of airtightness, no purification ability, radiation pollution, etc., and achieve the effects of good air permeability, improved strength and good permeability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0063] Dry the diatomite to remove impurities, put the cleaned diatomite into a rotary kiln for calcination at 900°C, and calcine until the silica content reaches 90%; add 5g of diatomite to 100g of calcined diatomite Zinc oxide was activated. After 40 minutes of activation, 1 g of octadecanoic acid was added for modification. After 40 minutes of modification, octadecanoic acid-modified diatomite was obtained.
Embodiment 2~5
[0065] Add nano-tourmaline powder, nano-titanium dioxide, inorganic gel powder and an appropriate amount of water to the octadecanoic acid-modified diatomite prepared in Example 1, and stir for 30 minutes to obtain a mixture. See Table 1 for the ratio of each raw material.
[0066] Table 1 Raw material ratio used in Examples 2 to 5 of the present invention
[0067]
[0068] The mixture is molded in a molding machine, and then dried in a dryer to obtain a diatomite composition.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
porosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com