A wet deoxidizer and dual-function technology, applied in the field of deoxidizers, can solve the problems of lack of dehumidification and deoxidation data, restrict the use of deoxidizers, etc., and achieve the effects of convenient industrial production, low production cost, and convenient addition and use.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] Weigh 0.02g of chloroplatinic acid, 1g of potassium chloride, 1.03g of water and 0.06g of concentrated sulfuric acid, mix the above-mentioned substances, add 7g of 100 mesh reduced iron powder, stir rapidly, and then add 0.4g of silicon dioxide, 0.6g of Activated carbon and 0.4g of carbon fiber are quickly mixed evenly to make a deoxidation component, which is quickly packed into a bag-shaped package made of three-layer non-woven wrapping paper, and 4.5g of calcium oxide is used as a dehumidification component. The packaging bag and the dehumidifying components are sealed in an airtight container to obtain the dehumidifying and deoxidizing agent.
[0028] Determination of performance of dual-function dehumidifying and deoxidizing agent. Specific method: put the prepared dehumidifying and deoxidizing agent in a sealed jar with a volume of 2.5L, and the jar is connected with an oxygen meter and a humidity meter, and record the oxygen concentration and humidity in the cont...
Embodiment 2
[0030] Weigh 0.004g of chloroplatinic acid, 0.5g of potassium chloride, 1.496g of water and 0.06g of concentrated sulfuric acid, mix the above-mentioned substances, add 5g of 100 mesh reduced iron powder, stir rapidly, and then add 0.4g of silicon dioxide, 0.4 G kaolin, 2.0g activated carbon, mixed quickly and evenly to make deoxidation component, quickly put the deoxidation component into a bag-shaped package made of three-layer non-woven wrapping paper, take 6.0g calcium oxide as the dehumidification component, Finally, the packaging bag and the dehumidifying components are sealed in an airtight container to obtain the dehumidifying and deoxidizing agent.
[0031] Determination of performance of dual-function dehumidifying and deoxidizing agent. Specific method: put the prepared dehumidifying and deoxidizing agent in a sealed jar with a volume of 2.5L, and the jar is connected with an oxygen meter and a humidity meter, and record the oxygen concentration and humidity in the ...
Embodiment 3
[0033] Weigh 0.156g copper sulfate pentahydrate, 0.6g potassium chloride, 0.6g sodium chloride, 1.25g water and 0.06g concentrated sulfuric acid, mix the above substances, add 6g 100 mesh reduced iron powder, stir quickly and evenly, and then add Mix 0.5g of diatomite and 1.5g of activated carbon quickly and evenly to make a deoxidation component, quickly put the deoxidation component into a bag-shaped package made of three-layer non-woven wrapping paper, take 5.0g of calcium oxide and 0.5 g silica gel is used as the dehumidifying component, and finally the packaging bag and the dehumidifying component are sealed in an airtight container to obtain a dehumidifying and deoxidizing agent.
[0034] Determination of performance of dual-function dehumidifying and deoxidizing agent. Specific method: put the prepared dehumidifying and deoxidizing agent in a sealed jar with a volume of 2.5L, and the jar is connected with an oxygen meter and a humidity meter, and record the oxygen conce...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com