Abstract
Description
technical field
[0001] The invention belongs to the fields of daily cleaning and sanitation cleaning, and in particular relates to a self-adhesive mastic remover and a preparation method thereof. Background technique
[0002] Since the 1930s, self-adhesive labels have been widely used in the packaging industry, commodity industry, daily chemical industry, Electronic and electrical industry, logistics industry, pharmaceutical industry and other industries are deeply loved by people. In particular, the emergence of self-adhesive advertisements has once again attracted people's attention in a new form of self-adhesive materials, and is more popular.
[0003] Self-adhesive materials have a wide range of uses and are convenient and quick to use. This is certainly an advantage, but the removal of self-adhesive glue is difficult, but it has become a headache. At present, various styles of self-adhesive small advertisements, incomplete self-adhesive signs, self-adhesive decoration...
Examples
Embodiment Construction
[0024] This aspect will be further described below in conjunction with an implementation case.
[0025] First, add 2g of PVA (polyvinyl alcohol) and 20g of water into the reactor and stir for 20 minutes. While stirring, raise the temperature to 80°C until the PVA (polyvinyl alcohol) is completely dissolved; then drop the temperature to 50°C and then add Fatty alcohol ether Phosphate monoester 6g, nonylphenol ether phosphate monoester ethanolamine salt 4g, a-alkenyl sulfonate 10g, bleaching powder 6g, carry out alcoholysis for 1-1.5 hours; cool down to 45°C and then add diethylene glycol monobutyl ether 12g, Triethylene glycol 10g, NMP 13g, after stirring and mixing evenly, then add 13g of light calcium carbonate, 15g of gypsum powder and 0.5g of other additives, after measuring its viscosity, add appropriate amount of colorant and essence, stir evenly, and finally add water to adjust its When the hardness is right, let it cool for later use.
[0026] When using, if there are ...