[0014] Antibacterial and wet-scratch-resistant paint for interior walls, including the following raw materials in parts by mass: 40-50 parts of styrene-acrylic emulsion, 0.5 parts of acrylic emulsion, 12 parts of silicon micropowder, 7 parts of titanium dioxide, 0.1 part of ethyl vanillin, Texanol alcohol ester 1 part, 0.2 part of HPMA, 5 parts of polyethylene glycol 200, 0.1 part of octylphenol polyoxyethylene ether, and 80 parts of deionized water.
[0015] The preparation method of the present invention: according to the mass ratio, add 80% deionized water in the paint mixing tank, stir and add acrylic acid emulsion, stir evenly, add ethyl vanillin, Texanol alcohol ester, HPMA, octylphenol polyoxygen Vinyl ether, stir evenly, add silicon micropowder and titanium dioxide in turn, stir evenly, add polyethylene glycol 200, stir well, add styrene-acrylic emulsion after dispersion and grinding, stir for 30min, add the remaining deionized water and stir evenly, that is, .
Embodiment 2
[0017] Antibacterial and wet-scratch-resistant paint for interior walls, including the following raw materials in parts by mass: 40-50 parts of styrene-acrylic emulsion, 1 part of acrylic emulsion, 18 parts of silicon micropowder, 12 parts of titanium dioxide, 0.2 parts of ethyl vanillin, Texanol alcohol ester 2 parts, 0.5 parts of zinc stearate, 6 parts of polyethylene glycol 200, 0.2 parts of octylphenol polyoxyethylene ether, and 90 parts of deionized water.
[0018] The preparation method of the present invention is the same as that of Example 1, and the raw materials of each component are as described above.
Embodiment 3
[0020] Antibacterial and wet-scratch-resistant paint for interior walls, including the following raw materials in parts by mass: 45 parts of styrene-acrylic emulsion, 0.6 part of acrylic emulsion, 16 parts of silicon micropowder, 10 parts of titanium dioxide, 0.15 part of ethyl vanillin, and 1.6 parts of Texanol alcohol ester , 0.3 parts of HPMA, 0.1 parts of zinc stearate, 5.4 parts of polyethylene glycol 200, 0.16 parts of octylphenol polyoxyethylene ether, and 85 parts of deionized water.
[0021] The preparation method of the present invention is the same as that of Example 1, and the raw materials of each component are as described above.
[0022]
[0023] The performance test of the finished product obtained in the present invention shows that its antibacterial rate to Escherichia coli can reach more than 99.85%, the antibacterial rate to Staphylococcus aureus can reach more than 99.92%, the number of times of wet rubbing resistance can reach 3100 times, the adhesion is ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com