Composition for treating scar and preparation method thereof
A composition and scar technology, which can be used in drug combinations, medical preparations with non-active ingredients, and medical preparations containing active ingredients, etc., can solve the problems of insignificant treatment effect, affect the appearance and beauty of the patient, and achieve recovery. Normal skin tone, improved scar appearance, increased cellular activity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0018] The preparation method of the composition for treating cicatrix of the present invention, comprises the following steps:
[0019] a) weighing each raw material according to the formula ratio;
[0020] b) Stir glycerol and polycarbophil fully, add 20-80% of the total amount of deionized water to swell for 18h-36h;
[0021] c) Stir carboxylated polyetherpolysiloxane, triethanolamine and remaining deionized water in a constant temperature vacuum homogenizer for 45min to 90min;
[0022] d) After the temperature drops, add the remaining material and stir for 5-15 minutes. After stirring, pour the material out of the pot into the filling machine for packaging, and sterilize it by Co60 irradiation.
Embodiment 1
[0025] A composition for treating scars, which consists of the following ingredients in parts by weight: 900 parts of carboxylated polyether polysiloxane, 18 parts of polycarbophil, 8 parts of lavender essential oil, 30 parts of asiaticoside, azone 9.52 parts, 3.81 parts of oleic acid, 6.67 parts of elemiic acid, 0.7 parts of allantoin, 350 parts of glycerol, 50 parts of triethanolamine, 5 parts of triclosan, and 8000 parts of deionized water. Its preparation method comprises the following steps:
[0026] a) Weigh each raw material according to the above-mentioned formula ratio;
[0027] b) Fully stir glycerol and polycarbophil, add 2000 parts of deionized water to swell for 18 hours;
[0028] c) Stir carboxylated polyetherpolysiloxane, triethanolamine and remaining deionized water in a constant temperature vacuum homogenizer for 45min;
[0029] d) After the temperature drops, add the rest of the material and stir for 5 minutes. After stirring, pour the material out of the p...
Embodiment 2
[0031] A composition for treating scars, which consists of the following ingredients in parts by weight: 1000 parts of carboxylated polyether polysiloxane, 20 parts of polycarbophil, 10 parts of lavender essential oil, 45 parts of asiaticoside, azone 20 parts, 8 parts of oleic acid, 14 parts of elemiic acid, 1.0 parts of allantoin, 420 parts of glycerol, 80 parts of triethanolamine, 8 parts of triclosan, and 8200 parts of deionized water. Its preparation method comprises the following steps:
[0032] a) Weigh each raw material according to the above-mentioned formula ratio;
[0033] b) Stir glycerol and polycarbophil fully, add 3500 parts of deionized water to swell for 25 hours;
[0034] c) Stir carboxylated polyether polysiloxane, triethanolamine and the remaining 4700 parts of deionized water in a constant temperature vacuum homogenizer for 60 min;
[0035] d) After the temperature drops, add the rest of the material and stir for 9 minutes. After stirring, pour the materi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com