Method for extracting copper from organic silicon scrap

An organosilicon and waste technology, applied in crucible furnaces, electric furnaces, rotary drum furnaces, etc., can solve the problems of unfavorable environmental protection, low copper purity and high copper content, and achieve the effect of solving recycling and environmental protection

Inactive Publication Date: 2014-02-05
LUZHOU NORTH CHEM IND
View PDF3 Cites 18 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] Nowadays, some domestic small manufacturers are also engaged in the production of extracting copper from organic silicon waste, but the production method is relatively rough. They just use acid to acidify the waste, and do not extract the cuprous and elemental copper in the waste deeply. The copper content in the waste slag after completion is still high, and the purity of copper is low, which is not conducive to environmental protection

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0044] Mix 100 parts of waste hydrochloric acid with 5 parts of soluble oxidant (hypochlorous acid) evenly; add 20 parts of waste contact body to the mixed waste hydrochloric acid and stir at a constant speed for 3 hours. After the reaction is completed, adjust the pH value with sodium carbonate for 4. Filter to obtain a blue-green transparent solution. Add 10 parts of nested iron wire, and stir the solution vigorously. After filtering, the copper powder is dried in a vacuum oven to obtain the product. After ICP element analysis, the Cu content is 99.3%, and the copper content in the waste residue is only 0.3%.

Embodiment 2

[0046] Same as Example 1, only the soluble oxidant in the spent acid was increased to 10 parts. The reaction time is shortened to 2 hours. The copper produced by this method is analyzed by ICP element, and the Cu content is 99.8%, and the copper content in the waste residue is only 0.1%.

Embodiment 3

[0048] Same as Example 1, just reduce the soluble oxidant in the spent acid to 1 part. The copper content in the copper powder that such method makes is 98.5%, but the copper content in the waste residue is 0.7%.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a method for extracting copper from an organic silicon scrap, and particularly discloses a method for extracting a copper simple substance from waste contact, pulp residue hydrolysis residue and waste acid water generated in production of an organic silicon monomer. The method comprises the following steps: a, grinding the waste contact and/or pulp residue hydrolysis residue; b, adding a soluble oxidant to a solution of hydrochloric acid, and then carrying out acidizing treatment on the grinded waste contact and/or pulp residue hydrolysis residue by using the solution of hydrochloric acid containing the soluble oxidant; c, neutralizing the acidized slurry by using an alkali compound, and adjusting into subacidity; d, filtering the neutralized slurry to obtain filtrate; e, displacing copper in the filtrate with active metal, and then drying to obtain the product. By adopting the method, the solution of hydrochloric acid containing the oxidant is utilized to acidize, so that the copper in the scrap is completely converted into divalent copper; the product is high in copper purity; the copper in the scrap is lower than 0.5%; the problems of copper recovery and environmental protection in an organic silicon production process are solved.

Description

technical field [0001] The invention belongs to the field of chemical industry, and relates to a method for extracting copper from organosilicon waste, in particular to a process for extracting copper elemental substance from waste contacts produced in the production of organosilicon monomers, pulp slag hydrolysis waste residue, and waste acid water. Reduce the harm of toxic heavy metals to the environment while realizing the reuse of resources. Background technique [0002] Organosilicon is known as industrial monosodium glutamate. Its influence on industry and our daily life is increasing day by day. The development of organosilicon in my country has begun since the 1950s, but in the past 10 years, my country's organosilicon has developed the fastest and has made the greatest technological progress. 10 years. With the development of my country's economy, the society's demand for organic silicon products is also increasing, and the production of organic silicon monomers is ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C22B7/00C22B15/00
Inventor 张文博李争鸣王勇武唐荣娟张莹徐志远
Owner LUZHOU NORTH CHEM IND
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products